nooneshere - 30-9-2018 at 11:42
Trying to locate one of these.. seems they're all 5K used and 10-15k minimum new. A little out of my park..
there has to be some smaller scale or consumer like product like this ? or perhaps a good spot I havent found with used ones that actually have all
the parts?
alot of the used ones have no vessel / container or top for the device..
nooneshere - 30-9-2018 at 12:07
ive seen some " fluid air coffee roasters" but I doubt these will actually be able to handle wet clay material without flooding and short circuiting
..
any alternatives to drying wet material ? perhaps a vac oven? any input for best achieving wet material drying ..
elementcollector1 - 30-9-2018 at 19:41
Forgive me, I'm not very familiar with the use of fluidized beds. Would a vacuum dessicator not suffice?