rasiel - 19-7-2018 at 11:08
Does anyone know a place one can buy silver and copper crystals? I know the process to grow them but don't have the inclination or time. And it
probably takes a lot of practice to get nice large ones.
Ras
Doped-Al2O3-fusion - 19-7-2018 at 11:52
As far as copper, I have two pieces I grew through electrolysis. The 2nd one I let grow for three weeks in a near neutral solution. Are you wanting
faceted crystals or dendritic?
*Edited with attached pictures.
These probably aren't even close fo what you are looking for. The thicker one was grown for close to a month on very low current. I was trying to
recover as much copper from solution as possible and having high purity, so there isn't anything super exciting about it.
The thinner and darker one was grown for over a week or up to two if I remember. It cleans up nice in hot vinegar.
[Edited on 19-7-2018 by Doped-Al2O3-fusion]
![20180719_125602.jpg - 1.9MB](http://www.sciencemadness.org/talk/files.php?pid=524615&aid=69478)
Herr Haber - 20-7-2018 at 03:17
If you want to drool over beautiful crystals, definitely check out Onyxmet.com
I know of no other like them.
Doped-Al2O3-fusion - 21-7-2018 at 16:08
I've got some copper sulfide I recently created. There are some microscopic faceted crystals of either a synthetic covellite or chalcocite structure
and composition. It's a nice indigo blue which makes me side with a majority of covellite.
![Cupic-faceted_06.jpg - 365kB](http://www.sciencemadness.org/talk/files.php?pid=525039&aid=69546)
[Edited on 22-7-2018 by Doped-Al2O3-fusion]
![macro.jpg - 428kB](http://www.sciencemadness.org/talk/files.php?pid=525039&aid=69548)