Sciencemadness Discussion Board

cant find half cell for redox flow cell

ReaktionChamber - 5-7-2018 at 02:40

hey guys,

I am currently working on my stack for my redox flow cell. Problem is that can't find any shop online which is offering this "special" flow half cell. On the following YT clip, u can see the half cell.

https://youtu.be/u1TYDh8QRIc?t=305

I am also glad to hear other ideas of building a redox flow stack.

Kind regards,

Reaktionchamber

XeonTheMGPony - 5-7-2018 at 04:17

Well I will keep a close eye on this as I often planned to make one.

I live off grid with lots of 1kL tanks so no shortage of storage capacity!

unionised - 5-7-2018 at 08:38

It looks like it was made from perspex sheet.

RustyRonny - 14-8-2018 at 05:34

Hi Reaktionchamber,

The half cell could likely be made from a plastic block by drilling down and then from the sides several times, the multiple holes allow the equal distribution of the electrolyte through the felt I would assume. Are you trying to make the same cell as shown in the video or another?