NEMO-Chemistry - 12-12-2017 at 18:28
I got 5ltr Ammonia arrive, its wrapped up like a mummy in black wrap, alarm bells went off and i undid some the wrap. The container looks like milk
bottle plastic, and its already a bit white!!
Had i known it was going to be sent like this I wouldnt have got so much. 5Ltr is kind of alot to find storage for, whats best to store it in? The
strength is 27% Ammonia according to the label.
Could i seal up empty wine bottles for now? The only good thing is my lab is literally colder than the fridge!
[Edited on 13-12-2017 by NEMO-Chemistry]
Vosoryx - 12-12-2017 at 20:04
I store mine in HDPE - works well enough.
NEMO-Chemistry - 12-12-2017 at 20:15
Will get a fuel type can tomorrow then, wrap the cap threads in PTFE. Cheers
Vosoryx - 12-12-2017 at 22:02
That would probably also work. Looking at this chart of compatibility I have, ammonia is not actually that hard to store.
![Ammonia compat..png - 38kB](http://www.sciencemadness.org/talk/files.php?pid=500239&aid=63241)