Sciencemadness Discussion Board

Complete Recycling of Zinc Carbon Batteries

explosive eddy - 30-12-2016 at 00:09

So, the goal of this experiment was to obtain manganese dioxide so I can make some themite with the end goal of obtaining a chunk of manganese. But, while i was doing this I decided to try and recycle every part from the battery including the casings and the electrolyte. See my experiment here. Subscribe to my youtube channel to see manganese thermite video in the future. https://www.youtube.com/watch?v=EezhK41G6ZM