Sciencemadness Discussion Board

Copper glycerol jelly ?

wg48 - 17-11-2016 at 04:49

I tried to make a Liesegang pattern with copper sulphate dissolved in glycerol and ammonia vapour. Not very successful. I added ammonia solution but just one ring formed and eventually the whole solution turned deep purple/blue. When I was about to dispose of the experiment I discoverd there was a deep purple blue coloured jelly at the bottom of the tube that looked like it contained crystals of the same color..

I removed the jelly. No crystals the jelly had fractured causing the appearance of crystals I dried it at 100C and some glycerol oozed from the jelly. It did not dissolve in the cold or hot water and is only slightly soluble in dilute NaOH. It does dissolve in dilute HCl to a light greenish solution.

On heating there is no obvious smell of ammonia but I did get a very acrid whiff of something. On heating below dull red heat the jelly decomposes with occasional pops to leave a black slight copper coloured deposit.

I speculate the jelly is a polymer copper glycerolate or more accurately a complex copper glycerol with sulphate as the counter ion and perhaps some ammonia.

I am trying to wash the jelly of any glycerol with acetone at present see the pic. The color is very very similar to copper sulphate hydrate.


Cugly.jpg - 36kB

Cryolite. - 17-11-2016 at 13:38

I have no idea about the complex, but the acrid whiff you caught was most likely acrolein formed by dehydration of the glycerol under catalysis by the copper.

wg48 - 18-11-2016 at 05:15

Quote: Originally posted by Cryolite.  
I have no idea about the complex, but the acrid whiff you caught was most likely acrolein formed by dehydration of the glycerol under catalysis by the copper.


Yes thats what I figured as well. Perhaps super acrid would have been more accurate. It certainly detered me from smelling it again and may have masked any smell of ammonia.

Glycerol is known to form complexes with copper at high pH thats probably what the jelly is. It may involve the ammonia too.

The jelly is air stable to 100C(pre acetone wash) and acetone wash stable. When incubated with water at 100C for a round 30min the jelly converts to a brown friable mass. Presumably copper oxide and or copper.

I just checked the container of jelly and it has a distinct smell of ammonia.

PHILOU Zrealone - 27-11-2016 at 11:23

By heating Pb(OH)2 with glycerol one can get lead-glycerolate

Pb(OH)2 + HOCH2-CHOH-CH2OH -heat-> *Pb-OCH2-CHO*-CH2OH + 2 H2O(g)

The compound is mildly explosive when heated dry into a hot flame.

I suspect Cu(OH)2 in NH4OH did the same kind of compound...

wg48 - 28-11-2016 at 06:32

Quote: Originally posted by PHILOU Zrealone  
By heating Pb(OH)2 with glycerol one can get lead-glycerolate

Pb(OH)2 + HOCH2-CHOH-CH2OH -heat-> *Pb-OCH2-CHO*-CH2OH + 2 H2O(g)

The compound is mildly explosive when heated dry into a hot flame.

I suspect Cu(OH)2 in NH4OH did the same kind of compound...


Yes I believe your correct. I was calling it a glycerol complex. as per this paper http://psasir.upm.edu.my/8995/1/FPP_1998_12_A.pdf

Incidently I placed a dry mixture NaOH and NH4OH wrapped up in a filter paper in the storage jar with the jelly to re-ammoniumate it . I thought since the jelly was dried and washed with acetone. the colour had significantly changed from midnight blue to a more copper sulphate blue.

Within minuts the colour of the jelly (or more accuratly crumble since it has been dryed and washed) turned a deep midnight blue and the surface appeared to be shiny more like the orginal jelly. Hours later it had partilly melted. Both the liquid and solid were now the dark midnight blue color.

Prevously I had only seen the copper complex (gylcerolate) in a solution. Perhaps in a more concentrated solution it forms a jelly.