Quote: Originally posted by FireLion3 ![](images/xpblue/lastpost.gif) | I checked, the density is definitely way off.
I checked with the supplier and they informed me that the purity of what I ordered was 99.1%, which could account for the inaccurate density.
|
It would take an 1% impurity of lead tetraethyl to change the density that much. My guess is that they bought it from China, and that means that they
have no idea what is in it. An NMR or GC MS would be the best way to test it, but that is not trivial. But even a TLC would help determine if it is
one compound or more. |