kazaa81 - 31-10-2004 at 15:25
Hallo to all,
after watched all the crap explanation about napalm and haven't finded anything clear about it, I've decided to write a clear description of
what it is.
In attachment I've post the description I've writed and some patents related.
Thanx at all. ![;)](./images/smilies/wink.gif)
Attachment error....
kazaa81 - 31-10-2004 at 15:29
Probably the file is too much big for only one attachment and, because of this, it hasn't been posted....
Attachment: Napalm by kazaa81.txt (5kB)
This file has been downloaded 1136 times
First related patent...
kazaa81 - 31-10-2004 at 15:31
First related patent about gelling agents...
Attachment: U.S. Patent 2,390,609.zip (152kB)
This file has been downloaded 663 times
Second related patent...
kazaa81 - 31-10-2004 at 15:36
Second related patent about gelling agents...
Attachment: U.S. Patent 2,618,536.zip (655kB)
This file has been downloaded 643 times
Third related patent...
kazaa81 - 31-10-2004 at 15:42
Third related patent about gelling agents...
Attachment: U.S. Patent 2,751,359.zip (888kB)
This file has been downloaded 651 times
sorry
Polverone - 31-10-2004 at 15:56
Napalm is not exotic enough to qualify for discussion here. As a rule, we don't discuss weapons, unless there is something novel or exotic about
their chemistry. Napalm is well-documented, though a lot of misinformation circulates on the web.