feacetech - 2-5-2013 at 13:51
I have a water shaker bath (20 C) that gets alot of red iron corrosion, the metal looks like stainless (I will confirm later)
after cleaning
would adding K2CrO4 and or Na2MoO4 help prevent this
how much would I add 100ppm of each?
and would it be wise to adjust the pH aswell to alkaline or acid state
feacetech - 2-5-2013 at 14:17
Hmmm scrap that after cleaning thers no visable corrison on the metal surfaces, its is probly just a brown bacterial sludge and built up tds from not
being drained frequently enough.