R.Esposito - 24-1-2013 at 08:01
Hi. I'm working with Raney Nickel (300g) and Pd/C 10% (10g). After two uses this catalyst no working. I wash some distilled water but this no good
results.
Please, how I clean and re-activate this mixture catalyst? Thanks for reply.
EdMeese - 25-1-2013 at 14:49
depends entirely on what you did with it, but lacking any and all details, first guess is to cook it. 300 °C in a 5%H2/N2 atmosphere maybe.
R.Esposito - 29-1-2013 at 01:34
Pd/C 10% can be cleaned by NaOH to pH 7. Palladium lost activity at the 2 times using.
Problem is mixture this 2 types of catalyst. I got some reference, must read and try.
zed - 29-1-2013 at 19:15
What are you doing with the catalyst? You didn't say.
Assuming it is hydrogenation. You could try cautiously soaking it in 3% hydrogen peroxide, with acetic acid, with warming.
This might partially reactivate your catalyst, or not.