I had quite a large batch of ‘high grade’ SnCl2.2H2O which turned out to be largely insoluble, presumably due to hydrolysis, perhaps also part oxidation to Sn(IV). In order not to waste the product completely I decided to convert it to SnO2.

The batch was mixed with about the same weight of water, stirred so that some of it dissolved and then strong ammonia was added to about neutral pH. The resulting slurry was filtered (it filtered easily) and washed with hot tap water, then hot DIW. (the filtrate still smelled faintly of NH3).

The filter cake was a light yellow sandy substance, presumably mostly Sn(OH)2.nH2O. It was dripped ‘dry’, then put in a defunct but clean, shallow aluminium pan and heated on an electrical plate. Right away the product started discolouring to grey. I thought this might be Al pick up and transferred the material to a Pyrex oven dish but on heating the discolouration continued: by that time the stuff was almost dark grey!

But low and behold, on further heating the colour reverted back to a much lighter colour, with patches of light yellow here and there. After a couple of hours, occasionally stirring and turning, the now dry product looked like the synthetic Cassiterite I bought from eBay some years back: off white to light grey.

I presume that during air oxidation of SnO an intermediate oxide of dark (black?) colour is formed, something like:

SnO + ½ O2 → SnO2
SnO + SnO2 → Sn2O3 (SnO.SnO2)
Sn2O3 + ½ O2 → 2 SnO2

Wiki mentions the formation of something like that on heating of SnO in inert atmosphere through disproportionation to Sn and SnO2 but here we are in oxidising conditions.


[Edited on 23-8-2012 by blogfast25]

[Edited on 23-8-2012 by blogfast25]

AJKOER - 23-8-2012 at 10:47

Interestingly, I was looking at an old and more recent sources and the reaction of SnCl2 with aqueous NH3 may result in compound salts, (NH4)2SnCl4 or even (NH4)2SnCl6, mixed in with the Sn(OH)2.

One possible undesirable reaction sequence:

SnCl2 + 2 NH3 + 2 H2O --> Sn(OH)2 + 2 NH4Cl

SnCl2 + 2 NH4Cl --> (NH4)2SnCl4

Or on net:

2 SnCl2 + 2 NH3 + 2 H2O --> Sn(OH)2 + (NH4)2SnCl4

Not knowing to what extent this or other reaction sequences could take place, I would not be surprised if the yield of SnO2 was less than expected.

Recent reference: "Competition Science Vision", Aug 2000, page 789.

Link: http://books.google.com/books?id=jegDAAAAMBAJ&pg=PA789&a...

Old Source: "Hand book of chemistry", Volume 5, by Leopold Gmelin, page 94.

Link: http://books.google.com/books?id=OgI5AAAAMAAJ&pg=PA94&am...


[Edited on 23-8-2012 by AJKOER]

unionised - 23-8-2012 at 11:23

I think it's disproportionation to Sn and SnO2.
At the surface the conditions are oxidising, but throughout the bulk material they are reducing.

blogfast25 - 23-8-2012 at 12:02

AJ:

I doubt if the NH3 played up. After washing only a trace remained. If there is such a complex (SnCl2.NH3) it could have slowed things down a bit, but not much more. On adding the strong NH3 to the slurry, no colour change was observed at all. That only happened on heating in air.


Quote: Originally posted by unionised  
I think it's disproportionation to Sn and SnO2.
At the surface the conditions are oxidising, but throughout the bulk material they are reducing.


Funnily enough, when it reverted back to 'normal' colour this happened FIRST at the bottom of the material. Of course that was also the hottest layer.

AJKOER - 23-8-2012 at 13:20

Blogfast25:

Upon further research, before seeing your comment, I removed the possible formations of the SnCl2.NH3 and SnCl2.2NH3 abducts as these may be created only by the anhydrous SnCl2 reacting with ammonia gas. Although I would not be surprised if these abducts, upon being created, were capable of forming hydrates (in a similar fashion to CaCl2).

However, per the reactions, for example:

6 SnCl2 + 2 H2O + O2 --> 2 SnCl4 + 4 Sn(OH)Cl (s)

SnCl2 + 2 NH3 + 2 H2O --> Sn(OH)2 + 2 NH4Cl

SnCl4 + 2 NH4Cl --> (NH4)2SnCl6 (Ammonium chlorostannate or pink salt)

any resulting formation of (NH4)2SnCl4 or even (NH4)2SnCl6, could reduce your yield of SnO2.

woelen - 23-8-2012 at 22:16

Isn't the dark color simply due to formation of SnO from Sn(OH)2? Subsequent change of color to white again is due to oxidation of SnO to SnO2.

SnO is a dark substance, nearly black. SnO2 is white. Sn(OH)2 also is white. So, these changes of color you observed are totally understandable.

blogfast25 - 24-8-2012 at 05:01

Quote: Originally posted by AJKOER  
Blogfast25:

Upon further research, before seeing your comment, I removed the possible formations of the SnCl2.NH3 and SnCl2.2NH3 abducts as these may be created only by the anhydrous SnCl2 reacting with ammonia gas. Although I would not be surprised if these abducts, upon being created, were capable of forming hydrates (in a similar fashion to CaCl2).

However, per the reactions, for example:

6 SnCl2 + 2 H2O + O2 --> 2 SnCl4 + 4 Sn(OH)Cl (s)

SnCl2 + 2 NH3 + 2 H2O --> Sn(OH)2 + 2 NH4Cl

SnCl4 + 2 NH4Cl --> (NH4)2SnCl6 (Ammonium chlorostannate or pink salt)

any resulting formation of (NH4)2SnCl4 or even (NH4)2SnCl6, could reduce your yield of SnO2.


Yep, I did think SnCl2 ammoniacates would only be formed in anhydrous conditions.

As regards pink salt, I made significant quantities of it a while back (it’s reported on this forum somewhere). It’s a white, crystalline water soluble compound that on strong heating completely sublimes (presumably to NH4Cl and SnCl4) leaving no trace. The trouble with your hypothesis though is that there’s precious little NH3 to begin with. The oxidation of Sn (II) to Sn (IV) in wet conditions in air is clearly slow. I didn’t measure yield quantitatively (impossible to do, as I didn’t really know what I started from) but the amount I obtained seemed reasonable, allowing also for the usual synthesis losses.
Quote: Originally posted by woelen  
Isn't the dark color simply due to formation of SnO from Sn(OH)2? Subsequent change of color to white again is due to oxidation of SnO to SnO2.

SnO is a dark substance, nearly black. SnO2 is white. Sn(OH)2 also is white. So, these changes of color you observed are totally understandable.

Woelen, I didn’t know SnO was black: the hydrated product is a light yellow, so I assumed SnO would be light coloured like SnO2. The discolouration started when the slurry was really quite wet still (it kind of ‘bumped’ badly at first). But it’s possible. Cu(OH)2 is blue and dehydrates to black CuO even when wet.

AJKOER - 24-8-2012 at 07:43

Quote: Originally posted by blogfast25  
Woelen, I didn’t know SnO was black: the hydrated product is a light yellow, so I assumed SnO would be light coloured like SnO2.


OK, per the source "A Text Book of Inorganic Chemistry", by Anil Kumar De, page 376, to quote:

"When freshly precipitated, the oxide has the composition 2SnO.2H2O. It is usually an olive-green powder which gives greyish crystals in contact with water."

Link:
http://books.google.com/books?id=PpTi_JAx7PgC&pg=PA379&lpg=PA379&dq=(NH4)2SnCl4+preparation&source=bl&ots=mp0VF3Nxrl&sig=pp8dW ha5AkWpxijaJDbt2X9qldM&hl=en#v=onepage&q&f=false
______________________________________

The SnO disproportionation alluded to previously is noted to occur in the solid state only. Per a Russian source, to quote (translation):

"Monoxide is produced by heating a solution of tin SnCl2 and alkali. In the solid state, it has a tendency to dismutation by the scheme:

2 SnO = SnO2 + Sn

but in the liquid (mp. 1040 ° C) and gas (bp. 1425 ° C) is stable. "

Link:
http://translate.google.com/translate?hl=en&sl=ru&tl...

I found another source ("Concise Encyclopedia Chemistry" by Walter de Gruyter) which notes a partial disproportionation to Sn and SnO2 upon melting at 1,080 C.


[Edited on 25-8-2012 by AJKOER]

blogfast25 - 24-8-2012 at 08:02

Quote: Originally posted by AJKOER  
Quote: Originally posted by blogfast25  
Woelen, I didn’t know SnO was black: the hydrated product is a light yellow, so I assumed SnO would be light coloured like SnO2.


OK, per the source "A Text Book of Inorganic Chemistry", by Anil Kumar De, page 376, to quote:

"When freshly precipitated, the oxide has the composition 2SnO.2H2O. It is usually an olive-green powder which gives greyish crystals in contact with water."

Link:
http://books.google.com/books?id=PpTi_JAx7PgC&pg=PA379&lpg=PA379&dq=(NH4)2SnCl4+preparation&source=bl&ots=mp0VF3Nxrl&sig=pp8dW ha5AkWpxijaJDbt2X9qldM&hl=en#v=onepage&q&f=false


Hmmm... I've precipitated "Sn(OH)2.nH2O" many times, also from really pure SnCl2 solutions, and have always obtained something off-white to light yellow. I might confirm this again with pix soon. Maybe even tonight.

blogfast25 - 24-8-2012 at 12:22

Below: a part ingot of 99.9 % Sn. Nice and shiny. Yum!

A bit of hack saw fun and 50 ml of 30 % iron free HCl later (the chunk of Sn reacting):


It took about 2 h to dissolve. The solution of SnCl2 was crystal clear and colourless.

Left tube: after adding strong NH3 to a few ml of the SnCl2 solution, Right tube, same treatment but with added 5 M NaOH (demonstrating amphoteric behaviour of Sn (II) - sodium stannite formed):



Now it gets really interesting. First up: the left hand tube emptied in a shallow pyrex dish (kitchen towel background): note how white the precipitate of ‘tin (II) hydroxide’ really is:



Then a time series, taken 2 – 3 mins apart with that dish on high heat on the hot plate:











Clearly the Sn (II) oxide hydrate dehydrates from white to brown/black before oxidation reverses the colour back to whitish tin (IV) oxide. During the run I could see crystalline structure being formed and the end-product shows crystalline areas too.



[Edited on 24-8-2012 by blogfast25]

AJKOER - 24-8-2012 at 17:00

Blogfast25:

Nice pictures!

Does the last picture show a touch of green and grey in places (hard to say)?

The next time you do this, I think it would be interesting to react SnCl2 with aqueous Na2CO3:

SnCl2 + Na2CO3 --> SnO (s) + 2 NaCl + CO2 (g)

and note whether the SnO looks the same. If it does not, I would not be too surprised as I would not normally describe a salt, as did my source (which I also saw described precisely the same way elsewhere) by its 'usual' color. Note, in the case of Al(OH)3 created via ammonia (actually this modification is called 'Aluminum oxide hydrate') bears no resemblance to Aluminum hydroxide via H2O2.

[Edited on 25-8-2012 by AJKOER]

blogfast25 - 25-8-2012 at 04:01

Quote: Originally posted by AJKOER  
Blogfast25:

Nice pictures!

Does the last picture show a touch of green and grey in places (hard to say)?

The next time you do this, I think it would be interesting to react SnCl2 with aqueous Na2CO3:

SnCl2 + Na2CO3 --> SnO (s) + 2 NaCl + CO2 (g)

and note whether the SnO looks the same. If it does not, I would not be too surprised as I would not normally describe a salt, as did my source (which I also saw described precisely the same way elsewhere) by its 'usual' color. Note, in the case of Al(OH)3 created via ammonia (actually this modification is called 'Aluminum oxide hydrate') bears no resemblance to Aluminum hydroxide via H2O2.

[Edited on 25-8-2012 by AJKOER]


No, that is a camera effect: the real thing is remarkably white, with the odd darker patch where oxidation hadn't completed yet. Lighting in my lab is far from optimal: 2 TL strip lights only leads to poor white balance.

I'll try the Na2CO3 route later on.

Not sure what you mean by 'Aluminum hydroxide via H2O2'...

[Edited on 25-8-2012 by blogfast25]

AJKOER - 25-8-2012 at 09:16

OK, I believe I did this experiment once. Slowly dissolve Al in Na2CO3.H2O2 (I used a generic Oxyclean brand). This resulted in a white amorphous and insoluble form of Al(OH)3.

If one tries this experiment with H2O2 and a strong base, the Al(OH)3 dissolves, but weak and the Al(OH)3 precipitates.

I will retry to verify, but unfortunately, this is not a quick reaction.

blogfast25 - 25-8-2012 at 13:32

This is the Sn (II) oxide hydrate from adding Na2CO3 saturated solution to yesterday’s SnCl2 solution:



Indistinguishable from the one made with NaOH with the naked eye. And white…Almost snow white…



[Edited on 25-8-2012 by blogfast25]

[Edited on 25-8-2012 by blogfast25]

Heuteufel - 26-8-2012 at 00:36

I once made SnO according to the procedure described in Brauer (precipitating hydrated tin(II)-oxide with Na2CO3 from SnCl2 and heating the hydrate on a NaCl-Water bath (110 °C). If the experiment is done right, beautiful blue-black cristals with metallic sheen are formed!:cool:
According to Brauer in air, SnO oxidized to SnO2 above 220 °C, a temperature easily achieved by a hotplate.
If you want to make SnO2 it is simplest to react Sn with nitric acid (attention:formation of copious amounts of NO2!).

blogfast25 - 26-8-2012 at 04:15

Quote: Originally posted by Heuteufel  
I once made SnO according to the procedure described in Brauer (precipitating hydrated tin(II)-oxide with Na2CO3 from SnCl2 and heating the hydrate on a NaCl-Water bath (110 °C). If the experiment is done right, beautiful blue-black cristals with metallic sheen are formed!:cool:
According to Brauer in air, SnO oxidized to SnO2 above 220 °C, a temperature easily achieved by a hotplate.
If you want to make SnO2 it is simplest to react Sn with nitric acid (attention:formation of copious amounts of NO2!).


Very interesting, Heuteufel. I will probably try that with the remaining SnCl2 solution.

Here the purpose was simply to salvage some SnCl2.2H2O 'gone bad'...

blogfast25 - 27-8-2012 at 11:07

Well, I tried to make anhydrous SnO but didn’t succeed, following Brauer’s method (drying hydrated SnO at 110 C, essentially).

I’d run out of Na2CO3, so for the first run I used NaHCO3 to neutralise the SnCl2 solution. Darkening started immediately but stopped at about olive green, after about 1 h on the sat. brine bath. 1 h later and no further darkening had occurred.

Then a test using strong NH3 but that SnO hydrate precipitate hardly darkened at all.

Perhaps it really is dependent on sodium carbonate as a neutralising agent to obtain a form of SnO hydrate that dehydrates slowly to anhydrous SnO at 110 C?


[Edited on 27-8-2012 by blogfast25]

S.C. Wack - 27-8-2012 at 15:50

Maybe it would be good to read what everyone was citing.

AJKOER - 27-8-2012 at 16:04

Quote: Originally posted by AJKOER  
OK, I believe I did this experiment once. Slowly dissolve Al in Na2CO3.H2O2 (I used a generic Oxyclean brand). This resulted in a white amorphous and insoluble form of Al(OH)3.

If one tries this experiment with H2O2 and a strong base, the Al(OH)3 dissolves, but weak and the Al(OH)3 precipitates.

I will retry to verify, but unfortunately, this is not a quick reaction.


Yes, in a few hours one has snow flakes in water ( Al(OH)3 ). A tip would be to quickly manually separate the snow flakes from the still visible strips of Al foil. In 2 days, the Aluminum strips have nearly completely broken down into black silicon specks and cannot be easily separated from the Al(OH)3.

For those interested in the chemistry, the Na2CO3 allows the penetration of the Al2O3 passive layer permitting a hydrolysis reaction:

2 Al + 6 H2O --> 2 Al(OH)3 (s) + 3 H2 (g)

blogfast25 - 28-8-2012 at 04:51

Quote: Originally posted by S.C. Wack  
Maybe it would be good to read what everyone was citing.


Huh? 'Splain, please SC?

S.C. Wack - 28-8-2012 at 15:18

Quote: Originally posted by blogfast25  
Huh? 'Splain, please SC?


Sometimes, even articles in German from 1922 have a word or three, somewhere, on why certain guidelines have to be followed?

blogfast25 - 29-8-2012 at 04:02

Quote: Originally posted by S.C. Wack  
Quote: Originally posted by blogfast25  
Huh? 'Splain, please SC?


Sometimes, even articles in German from 1922 have a word or three, somewhere, on why certain guidelines have to be followed?


Ok SC, you can quit speaking in tongues now.

Here’s the German abstract in your link:

”1. Es wurde das Gleichgewicht der Reaktion SnO2 + 2CO ⇋ Sn + 2CO3 [sic] studiert und gefunden, daß dieses Gleichgewicht von beiden Seiten her erreichbar und von Menge und Zusammensetzung des Bondenkörpers unabhängig ist.”

Says nothing relevant to synth of SnO. I’ll be trying that again this WE, this time using Na2CO3 as a base.

AJKOER - 29-8-2012 at 05:45

Here is some interesting material per Wiki:

"Blue-black SnO can be prepared by heating the tin(II) oxide hydrate, SnO.xH2O (x<1) precipitated when a tin(II) salt is reacted with an alkali hydroxide such as NaOH.[3] Metastable, red SnO can be prepared by gentle heating of the precipitate produced by the action of aqueous ammonia on a tin(II) salt.[3] SnO may be prepared as a pure substance in the laboratory, by controlled heating of tin(II) oxalate (stannous oxalate) in the absence of air.[4]

SnC2O4 → SnO + CO2 + CO

Tin(II) oxide burns in air with a dim green flame to form SnO2.[3]

2 SnO + O2 → 2 SnO2

When heated in an inert atmosphere initially disproportionation occurs giving Sn metal and Sn3O4 which further reacts to give SnO2 and Sn metal.[3]

4SnO → Sn3O4 + Sn
Sn3O4 → 2SnO2 + Sn

SnO is amphoteric, dissolving in strong acid to give tin(II) salts and in strong base to give stannites containing Sn(OH)3−.[3] It also dissolves in strong acid solutions to give the ionic complexes Sn(OH2)32+ and Sn(OH)(OH2)2+, and in less acid solutions to give Sn3(OH)42+.[3]"
Link: http://en.wikipedia.org/wiki/Tin(II)_oxide

Interestingly, a key phrase above on the preparation of red SnO via ammonia may be 'gentle heating'. Also, the statement that SnO is amphoteric may be significant.
____________________________________________

On SnCl2, again per Wiki:

"Tin(II) chloride can dissolve in less than its own mass of water without apparent decomposition, but as the solution is diluted hydrolysis occurs to form an insoluble basic salt:

SnCl2 (aq) + H2O (l) <==> Sn(OH)Cl (s) + HCl (aq)

Therefore if clear solutions of tin(II) chloride are to be used, it must be dissolved in hydrochloric acid (typically of the same or greater molarity as the stannous chloride) to maintain the equilibrium towards the left-hand side (using Le Chatelier's principle). Solutions of SnCl2 are also unstable towards oxidation by the air:

6 SnCl2 (aq) + O2 (g) + 2 H2O (l) → 2 SnCl4 (aq) + 4 Sn(OH)Cl (s)

This can be prevented by storing the solution over lumps of tin metal.[2]"

Also, the following comment "Tin(II) chloride also behaves as a Lewis acid, forming complexes with ligands such as chloride ion, for example:

SnCl2 (aq) + CsCl (aq) → CsSnCl3 (aq)

Most of these complexes are pyramidal, and since complexes such as SnCl3 have a full octet, there is little tendency to add more than one ligand. The lone pair of electrons in such complexes is available for bonding, however, and therefore the complex itself can act as a Lewis base or ligand."
Link: http://en.wikipedia.org/wiki/SnCl2

My take from the above is that SnCl2 with a dilute ammonia solution could form Sn(OH)Cl and further complex.

blogfast25 - 29-8-2012 at 07:00

Quote: Originally posted by AJKOER  

My take from the above is that SnCl2 with a dilute ammonia solution could form Sn(OH)Cl and further complex.


It's possible but in this run the ammonia was actually 25 - 30 % and an excess of it was used. Alkalinoty should really be high enough to hydrolyse all the way down to 'Sn(OH)2.nH2O', IMHO.

S.C. Wack - 29-8-2012 at 12:26

Quote: Originally posted by blogfast25  
Ok SC, you can quit speaking in tongues now.

Here’s the German abstract in your link:


I don't care what the abstract says? I'm obviously talking about the article itself cited by your reference, and also mine (which also mentions Ann. chim. phys.[5] 27, 145 (1882), attached hot and unread from gallica's press) which I don't have, and linked to? I'll download the large narod archive that it's in (at some point) but there is other downloading on my near-Luddite internet.

Attachment: N0034867_PDF_143_180DM.pdf (779kB)
This file has been downloaded 674 times


blogfast25 - 29-8-2012 at 13:00

SC, I’m sorry but you’ve still lost me: I didn’t link to anything. Instead I looked it up in Brauer and used first NaHCO3, then NH3 (aq) as source of alkalinity to precipitate the hydrated Sn (II) oxide, instead of Brauer’s recommended Na2CO3. Neither of my tests succeeded in making brown/black anhydrous SnO.

The French pdf however is interesting in the sense that it actually recommends NH3 (aq) as the base and that on heating to 110 C the anhydrous material can be obtained. So thanks for that.

I think I’ll try this again, this time replacing the supernatant mix of NH4Cl and NH3 by clean water. After all, when converting the faulty SnCl2 that’s what I did and discolouration on heating took place immediately.

S.C. Wack - 29-8-2012 at 14:24

Quote: Originally posted by blogfast25  
SC, I’m sorry but you’ve still lost me: I didn’t link to anything.


I didn't say anywhere that you linked to anything? Is all this some kind of joke?

blogfast25 - 30-8-2012 at 04:11

No SC, it just seems we've got our wires crossed.

S.C. Wack - 31-8-2012 at 13:42

12.6 GB later...F&S's Z. anorg. article says nothing more, except that they are following Ditte's guidelines. It's not worth posting I guess. Everyone cites F&S (Brauer) as the way to go (the J. Phys. Chem. reference mistakenly gives all the credit to the French article, which they must not have read). But one of the other Z. anorg. references does a few experiments. So, instead:

Attachment: z_anorg_213_301_1933.pdf (258kB)
This file has been downloaded 616 times

[Edited on 31-8-2012 by S.C. Wack]

blogfast25 - 1-9-2012 at 13:07

Quote: Originally posted by S.C. Wack  
12.6 GB later...F&S's Z. anorg. article says nothing more, except that they are following Ditte's guidelines. It's not worth posting I guess. Everyone cites F&S (Brauer) as the way to go (the J. Phys. Chem. reference mistakenly gives all the credit to the French article, which they must not have read). But one of the other Z. anorg. references does a few experiments. So, instead:



[Edited on 31-8-2012 by S.C. Wack]


That text seems like an interesting monography on SnO, quite complete state of the art, at least up to that moment in time. Thank you.

AJKOER - 13-10-2012 at 13:27

Here is a new source (link: http://tin.atomistry.com/stannous_oxide.html ) with interesting comments on forming SnO. To quote:

"Stannous Oxide, SnO, may be prepared in several ways. It is obtained by heating a mixture of stannous chloride and sodium carbonate until it becomes black, then washing with water, and drying the residue with a gentle heat in a stream of carbon dioxide. It is also produced by igniting stannous oxalate out of contact with air, when it is obtained as an olive-green powder; and by precipitating stannous chloride solution with alkali, and boiling the hydrated oxide thus produced with dilute caustic potash solution; the anhydrous oxide thus formed crystallises in microscopic cubes or octahedra. A crystalline form of the oxide is also obtained by digesting a nearly saturated solution of stannous oxide in acetic acid of density 1.06 at 56° C. This form of the oxide is red, but quiokly turns black on exposure to sunlight.

The black amorphous oxide easily dissolves in hydrochloric acid forming stannous chloride, and burns when heated in the air forming the dioxide:

SnO(cryst.) + ½O2 = SnO2(cryst.) + 71,000 calories"