ftirinih - 19-7-2012 at 16:28
I pulled this out of a Bomem MB 120 spectrometer. I'd like to replace it with fresh desiccant but I don't know what this is. It is probably a common
type. Temporarily I put in some clay desiccant in its place. Does anyone know what type of desiccant this is?
![desiccant.jpg - 131kB](http://www.sciencemadness.org/talk/files.php?pid=254874&aid=19572)
zoombafu - 19-7-2012 at 17:11
Looks like it could be Drierite. https://secure.drierite.com/catalog3/page4b.cfm?
jamit - 19-7-2012 at 18:51
I agree with zoomfad ...It looks like drierite!
vmelkon - 20-7-2012 at 03:52
If it is drierite, then it is CaSO4 + some CoCl2.
You can get rid of the water of hydration by heating it. Do a test on a small sample and see if it works.