GreenD - 29-4-2012 at 09:53

Anyone know how to fix this?

I thought if I was careful and kept the ground glass dry I wouldn't have a problem. Well that is nearly impossible, and my glass joint is basically stuck.

Any help?

kristofvagyok - 29-4-2012 at 10:15

Quote: Originally posted by GreenD  

Any help?


Hammertime!:D

Seriously: heat it up to 100-150C and sometimes it come out. Or try to hit it a littlebit to a table and maybe it will release....