metalresearcher - 19-4-2012 at 12:31
With an electric welder I made an arc which melted MgO rods like plastic ....
<iframe sandbox width="760" height="465" src="http://www.youtube.com/embed/AHAUHIOD_5Y" frameborder="0" allowfullscreen></iframe>
vmelkon - 20-4-2012 at 06:26
That's neat. Perhaps you can make a MgO crucible.