Quote: Originally posted by peach ![](images/xpblue/lastpost.gif) | NaCl can be dried out by simply roasting the shit out of it in the open atmosphere. This is a standard chef trick for salt baked fish.
|
I'm not sure what this thread is about, but note that NaCl is not hygroscopic, so "heating the shit out of it" seems a bit of an overkill. Actually
I'm not aware of any NaCl hydrates. If your chef's table salt cakes, the most likely cause is that there are alkaline earth metal chlorides inside.