Originally posted by dann2
Hello,
Quote: | Originally posted by Rosco Bodine
@Xenoid
I felt the need to have a cool breeze blow through and leave some extra cool across this page before I blow my own Paul Simon seemed appropriate to the moment .
|
Try the pills and Absolute ethanol, always works for me ![:D](./images/smilies/biggrin.gif)
You'll be looking for them after listening to that shit, .................(ONLY JOKING).
Quote: | Originally posted by Rosco Bodine
@dann2 , [snip]
you are certain don't exist , because we aren't even on the same page concerning ATO , how it works , proportions , precursors , interpreting
measurements ,
|
My bottom line on the information for DTO for anodes is that I am much, much, much more inclined to follow DTO information that is presented in Anode
patents, as opposed to DTO information regarding applications for making resistors/conductors on glass and other non conductive substrates and other
time consuming speculation. |