Cobalt Oxide Anodes Dann2 maybe with your DTO coatings you've already got the answer.
Could you explain the details o ... |
6-12-2007 at 17:02 by: jpsmith123 |
Some Papers I'd Like To Look At I wonder if anyone has access to the following papers? These sound like they may have some useful in ... |
6-12-2007 at 12:22 by: jpsmith123 |
Cobalt Oxide Anodes Xenoid the way you describe your baked on coating...well it sounds exactly like my best electrodepos ... |
6-12-2007 at 09:16 by: jpsmith123 |
Cobalt Oxide Anodes Xenoid with regard to your baked on coating, I'm trying to get an idea of how well it stuck to the t ... |
5-12-2007 at 19:52 by: jpsmith123 |
Cobalt Oxide Anodes [quote][i]Originally posted by Xenoid[/i]
Yes, but CoO is not desirable, we want Co3O4 in the spine ... |
5-12-2007 at 18:52 by: jpsmith123 |
Cobalt Oxide Anodes Hello Chloric1,
Co Acetate apparently does decompose in air to CoO.
J. Mater. Chem., 1991, 1 ... |
5-12-2007 at 17:24 by: jpsmith123 |
Cobalt Oxide Anodes Well the Co Acetate solution doesn't work too well for painting and baking...it's just not soluble e ... |
5-12-2007 at 16:41 by: jpsmith123 |
Cobalt Oxide Anodes Yeah, I know that particular patent specifically says "TiOx where x = .45 to 1.2 and preferably wher ... |
5-12-2007 at 02:38 by: jpsmith123 |
Cobalt Oxide Anodes Mmmm...doesn't that look tasty! And to make it even better, I suggest adding some powdered sugar, er ... |
4-12-2007 at 17:08 by: jpsmith123 |
Cobalt Oxide Anodes Dann2 I went back and read that part of the thread, and you're right, he does sound legitimate.
... |
4-12-2007 at 06:00 by: jpsmith123 |
Cobalt Oxide Anodes If you can heat to about 300 degrees C, the acetate should work nicely, as it is highly soluble in w ... |
3-12-2007 at 15:56 by: jpsmith123 |
Cobalt Oxide Anodes So Dann2 you're done experimenting with cobalt? You're not going to try any kind of baked on coating ... |
3-12-2007 at 12:12 by: jpsmith123 |
Cobalt Oxide Anodes I'm glad to hear that it's still running.
If you make another, I'd like to suggest adding some T ... |
3-12-2007 at 09:52 by: jpsmith123 |
I give up on the electrodeposition idea. Well let's see, three of us tried it...to no avail. I tried putting it over graphite, platinum, TiH2 ... |
3-12-2007 at 05:56 by: jpsmith123 |
Cobalt Oxide Anodes As per Xenoid's suggestion...
And I'll open the discussion with this:
The electrodeposition of ... |
2-12-2007 at 20:31 by: jpsmith123 |
TiH2 Substrates Rosco do you know if TiH2 can be soldered? I thought I remembered reading somewhere that it could be ... |
2-12-2007 at 20:04 by: jpsmith123 |
More on PbO2 electrodes Making it go from 250 to 500 C sounds more like "redesign" than "modification" .
Anyway, what I ... |
2-12-2007 at 19:43 by: jpsmith123 |
More on PbO2 electrodes How hot can a toaster oven get? I didn't think they would go much over 250 degrees C, which is proba ... |
2-12-2007 at 19:03 by: jpsmith123 |
More on PbO2 electrodes Xenoid my first sample ran for a little while, then, shortly after I noticed some black stuff floati ... |
2-12-2007 at 17:06 by: jpsmith123 |
TiH2 Substrates Well the hydriding in acetic acid didn't work too well. I couldn't deposit cobalt oxide over it.
... |
2-12-2007 at 09:46 by: jpsmith123 |
More on PbO2 electrodes [quote]
How might one make Co Nitrate from Co Sulphate?
[/quote]
According to one of the handbo ... |
2-12-2007 at 05:42 by: jpsmith123 |
TiH2 Substrates Probably the metal is deposited on the negative half-cycle and oxidized on the positive half-cycle.
... |
30-11-2007 at 18:50 by: jpsmith123 |
TiH2 Substrates Yep I was getting quite a lot of bubbles.
BTW, earlier today I cathodized another piece of Ti wir ... |
30-11-2007 at 17:02 by: jpsmith123 |
Another Hydride Related Patent The attached patent describes a "Process For Electro-plating Nickel On Titanium".
In this case t ... |
30-11-2007 at 10:20 by: jpsmith123 |
How thick can an anodized layer be? Hello Tacho,
I admire your resourcefulness, but is it worth it to even fool around like that when ... |
30-11-2007 at 09:16 by: jpsmith123 |