Search |
[Next Page] |
Smoke Formulations ( book excerpt) Traditionally US military white smokes have been powdered zinc and hexachloroethane (such as used in ... |
29-3-2008 at 11:02 by: Sauron |
NaOH solution density Well, that seems to be wrong. Because a liter at d = 1.55 is 1550 g and 52.2% of 1550 g is certainly ... |
29-3-2008 at 10:19 by: Sauron |
NaOH solution density Yes, thanks. I certainly did not mean to ridicule the Baume scales, they still pop up from time to t ... |
29-3-2008 at 09:36 by: Sauron |
NaOH solution density I am looking at an older text from the forum library "Fundamental Processess of Dye Chemistry" which ... |
29-3-2008 at 08:46 by: Sauron |
Anyone have Practical Experience with Polymer Synthesis? An Auspicious Beginning
I need a 4 liter cylindrical Morton (baffled) reaction vessel for this an ... |
28-3-2008 at 10:00 by: Sauron |
NaOCl Actually, according to Brauer (see attached) crystalline NaOCl.5H20 is isolable, and its solubility ... |
28-3-2008 at 06:36 by: Sauron |
AIBN Preparation: 2 Steps from Acetone The following is cortesy of garage chemist. It is the original preparation of hydrazibisisobutyronit ... |
28-3-2008 at 03:10 by: Sauron |
Anyone have Practical Experience with Polymer Synthesis? I have a couple of practical questions.
1. Is it necessary to use a cylindrical vessel, or will a ... |
27-3-2008 at 08:08 by: Sauron |
AIBN Preparation: 2 Steps from Acetone I'll be appending this as time goes by, adding the alternative route from acetone cyanohidrin, and t ... |
27-3-2008 at 06:06 by: Sauron |
AIBN Preparation: 2 Steps from Acetone Preparation of AIBN Azobis(isobutyronitrile)
The virtues of this preparation are simplicity, abse ... |
26-3-2008 at 07:19 by: Sauron |
Adios I am ceasing to post here.
The environment on the forum has become unendurable for me.
I have ... |
12-3-2008 at 03:53 by: Sauron |
Electrolysis of aqueous SO2 yeilding H2SO4 The nomenclature (old style) is ass-backwards, but the molecular formulas are straightforward.
T ... |
12-3-2008 at 02:41 by: Sauron |
post whores like me Nicodem, I must demurr. My sole comment directed to Ephoto was:
Let sleeping threads lie.
Whic ... |
11-3-2008 at 11:27 by: Sauron |
Melatonin: 5-MeO-N-Acetyltryptamine I posted the Organic Reactions chapter on the Japp-Klingmann reaction some time back as it is part o ... |
11-3-2008 at 11:11 by: Sauron |
Electrolysis of aqueous SO2 yeilding H2SO4 Well, no. SOCl2 is produced by oxidizing SCl2 and/or S2Cl2 with SO3, neat or in high % (>60%) ole ... |
11-3-2008 at 10:31 by: Sauron |
post whores like me To be fair there does seem to be confusion as there IS a Pamona community college but the official n ... |
11-3-2008 at 10:20 by: Sauron |
Melatonin: 5-MeO-N-Acetyltryptamine The thread is about melatonin, a nutraceutical. It is inappropriate to derail it to discuss 5-MeO-D ... |
11-3-2008 at 09:35 by: Sauron |
Melatonin: 5-MeO-N-Acetyltryptamine Forgive the repeat post without an intervening reply. Here is the reaction scheme from the 3-bromopr ... |
11-3-2008 at 09:14 by: Sauron |
post whores like me Actually. yesterday all I did was to question the thread author's spelling of Pamona, California (th ... |
11-3-2008 at 07:14 by: Sauron |
post whores like me You'd like some of us to drill holes in our heads and let some knowledge, education and experience l ... |
11-3-2008 at 04:00 by: Sauron |
Melatonin: 5-MeO-N-Acetyltryptamine Quite Alternative Route
US Patent 5,122,535 details the preparation of melatonin from p-anisidine ... |
11-3-2008 at 03:42 by: Sauron |
Melatonin: 5-MeO-N-Acetyltryptamine Although the Org.Syn.prep posted above employs overpriced potassium metal to prepare t-BuOK, constit ... |
11-3-2008 at 01:20 by: Sauron |
Melatonin: 5-MeO-N-Acetyltryptamine I dunno about the yohimbine structure as I honestly have forgotten what it looks like.
As you pro ... |
10-3-2008 at 22:07 by: Sauron |
Melatonin: 5-MeO-N-Acetyltryptamine I looked at this sort of thing a long, long time ago and have paid scant attention to it since.
T ... |
10-3-2008 at 20:53 by: Sauron |
Melatonin: 5-MeO-N-Acetyltryptamine This ubiquitous hormone was a bit of a health food fad a while back I think it is OTC. It used to be ... |
10-3-2008 at 20:32 by: Sauron |
[Next Page] |