Unified Copper Process Well, I've already got it to where I can generate H2S on demand. The reactions of chlorine and H2S ... |
29-6-2008 at 16:21 by: kilowatt |
Unified Copper Process After some experimenting I am leaning towards a calcium sulfide route to the SO2 for this process fr ... |
28-6-2008 at 18:45 by: kilowatt |
Condensing chlorine gas, price of ethane!!!! I think once you sell them, you will later find that you really did need them, and regret selling th ... |
18-6-2008 at 19:43 by: kilowatt |
Condensing chlorine gas, price of ethane!!!! If it goes to -85°C then you can use it to make dry ice by condensing CO2 from a tank or even as it ... |
18-6-2008 at 15:50 by: kilowatt |
Recasting teflon There is a fine line between melting and decomposition (to deadly gases such as HF and fluorophosgen ... |
13-6-2008 at 15:16 by: kilowatt |
Glass or teflon stop cock? [quote]
I don't have access to a torch, so I cant really heat just the outside joint.[/quote]
Just ... |
13-6-2008 at 08:59 by: kilowatt |
Glass or teflon stop cock? Teflon stopcocks shrink and expand greatly with temperature, and as such can easily come loose if th ... |
12-6-2008 at 20:21 by: kilowatt |
Easy production of ammonia? [quote]
haha... funny story, i don't know of any ammonium products that I can get my hands on... or ... |
31-5-2008 at 01:21 by: kilowatt |
Sword Forging! Did you pay extra for the premium sword quenched in elf blood or something? No mortal sword can cut ... |
17-5-2008 at 14:35 by: kilowatt |
Sword Forging! He is being sarcastic. A good sword would just bounce off all those items (and chip the edge) if it ... |
17-5-2008 at 11:04 by: kilowatt |
Barium Metal I would just coat it in thick wax and cut it with a hand saw of whatever type. If the shavings are ... |
16-5-2008 at 09:43 by: kilowatt |
Sword Forging! [quote]
All of them are steel alloys, and no other metals can compare[/quote]
There are some nicke ... |
15-5-2008 at 05:20 by: kilowatt |
Unified Copper Process Does CaB4O7 have any uses that might interest me? |
14-5-2008 at 17:05 by: kilowatt |
Unified Copper Process [quote]
I'm not sure if Ca2SiO4 exists and what its properties are. [/quote]
Ca2SiO4 is calcium or ... |
14-5-2008 at 15:23 by: kilowatt |
Unified Copper Process I have begun to experiment with the reaction of calcium sulfate with carbon and silica at high tempe ... |
14-5-2008 at 10:13 by: kilowatt |
PVD at home [quote]
Is terra cotta a suitable refractory material or am I living in dreamland?[/quote]
Maybe; ... |
13-5-2008 at 21:25 by: kilowatt |
Separation of Copper/Nickel Alloy [quote]
Copper sulfate decomposes to the oxide at about 650 C, nickel sulfate at about 850 C. If th ... |
19-4-2008 at 13:15 by: kilowatt |
worst stench I have a friend that works at the local apiary, and would often come home smelling like butyric acid ... |
18-4-2008 at 15:23 by: kilowatt |
Separation of Copper/Nickel Alloy [quote]
Otherwise, isn't one of 'em magnetic?[/quote]
Only in metallic form, below its austenitic ... |
18-4-2008 at 09:30 by: kilowatt |
Separation of Copper/Nickel Alloy [quote]
It would seem an easy task to dissolve the metals as a sulfate with an electrolytic cell, u ... |
17-4-2008 at 22:47 by: kilowatt |
Unified Copper Process Copper(I) chloride precipitates out when copper(II) chloride reduced by sulfite, but I am aware that ... |
17-4-2008 at 22:12 by: kilowatt |
Unified Copper Process I know of nowhere where I can buy sulfur for anywhere near the price of gypsum (I can get scrap dryw ... |
17-4-2008 at 21:47 by: kilowatt |
Separation of Copper/Nickel Alloy It would be pretty hard to leech all the copper out with ammonia I think, much as it would be pretty ... |
17-4-2008 at 21:16 by: kilowatt |
Separation of Copper/Nickel Alloy That copper (II) aspirinate looks really promising, fast and easy, and high yield as long as nickel ... |
17-4-2008 at 20:26 by: kilowatt |
Unified Copper Process I may have come up with a relatively straightforward process that unites the production of sodium hy ... |
17-4-2008 at 19:27 by: kilowatt |