Quest for the elements Electrolysis of a LiCl/KCl eutectic (MP about 300 C), not very well executed:
https://www.youtube ... |
14-10-2015 at 15:32 by: blogfast25 |
Quest for the elements [rquote=423159&tid=63794&author=Upsilon]
Honestly I think I'll go with the carbothermic. I ... |
14-10-2015 at 10:28 by: blogfast25 |
Quest for the elements [rquote=423098&tid=63794&author=j_sum1]I was thinking of perhaps a half kilo batch.[/rquote] ... |
14-10-2015 at 07:06 by: blogfast25 |
Quest for the elements [rquote=423094&tid=63794&author=Upsilon]
Does it occur with explosive force or something? W ... |
14-10-2015 at 07:03 by: blogfast25 |
Quest for the elements [rquote=423092&tid=63794&author=Upsilon]
That being said, I honestly have no idea what el ... |
13-10-2015 at 18:37 by: blogfast25 |
Quest for the elements [rquote=423078&tid=63794&author=Upsilon]So I recovered the pieces a little while ago. Upon a ... |
13-10-2015 at 17:33 by: blogfast25 |
Quest for the elements [rquote=422961&tid=63794&author=j_sum1]Thanks for reminding me how smelly this one gets. I ... |
13-10-2015 at 08:06 by: blogfast25 |
Quantum Mechanics/Wave Mechanics in Chemistry Beginners Thread [rquote=422928&tid=62973&author=aga]Gimme a sleep cycle and it'll all be assimilated.[/rquot ... |
12-10-2015 at 17:03 by: blogfast25 |
Quantum Mechanics/Wave Mechanics in Chemistry Beginners Thread [rquote=422884&tid=62973&author=aga]Gulp !
[/rquote]
Trouble in paradise? |
12-10-2015 at 15:03 by: blogfast25 |
Tungsten hexachloride production and its hydrolysis WCl<sub>6</sub> can't be prepared by trying to dissolve W in HCl, not even remotely. Onl ... |
12-10-2015 at 08:11 by: blogfast25 |
Quest for the elements [rquote=422816&tid=63794&author=woelen]
LiCO3 is a very special salt, which only exists i ... |
12-10-2015 at 06:17 by: blogfast25 |
Quest for the elements [rquote=422780&tid=63794&author=Upsilon]
I figured as much. I guess the small mixtures ju ... |
11-10-2015 at 17:53 by: blogfast25 |
Quest for the elements @Upsilon:
These very small amounts don't work well. Minimum 100 g of mix (approx.). Small amounts ... |
11-10-2015 at 17:38 by: blogfast25 |
K metal from KOH, Mg, and Diacetone Alcohol [rquote=422743&tid=63926&author=j_sum1]Paraffin oils are a bit hit and miss. The oil needs ... |
11-10-2015 at 15:45 by: blogfast25 |
K metal from KOH, Mg, and Diacetone Alcohol [rquote=422739&tid=63926&author=runninfarmer]I've been studying this Nurdrage video here: ht ... |
11-10-2015 at 15:35 by: blogfast25 |
Quantum Mechanics/Wave Mechanics in Chemistry Beginners Thread [b]Born-Haber Thermochemical cycle: Ionisation Energy, Electron Affinity and Lattice Energy:[/b]
... |
11-10-2015 at 13:23 by: blogfast25 |
Quantum Mechanics/Wave Mechanics in Chemistry Beginners Thread [rquote=422636&tid=62973&author=aga]Maybe, let's see.
Electronegativity is a measure of h ... |
11-10-2015 at 07:14 by: blogfast25 |
Quantum Mechanics/Wave Mechanics in Chemistry Beginners Thread Did the soaking bring any clarity, or are clarifications required, Squire? |
10-10-2015 at 17:05 by: blogfast25 |
Thinking in different number bases... Chinese multiplication:
https://www.youtube.com/watch?v=U2UloHO5Ubc |
10-10-2015 at 17:03 by: blogfast25 |
Thinking in different number bases... [rquote=422547&tid=63896&author=aga]Digital ? Dunno what that is.
8 is 1000 in Binary (ak ... |
10-10-2015 at 08:37 by: blogfast25 |
Tin and Zinc Chloride Synthesis For what it's worth (not that much), google images for tin chloride, mostly white:
https://www.go ... |
10-10-2015 at 08:32 by: blogfast25 |
Thinking in different number bases... [rquote=422501&tid=63896&author=aga]00000000000000000000000000000000000000000000000000000000 ... |
10-10-2015 at 08:01 by: blogfast25 |
[Next Page] |