Digital pH meters for sale Thanks Doc B, the only other time I would use one is for an AB extraction. But I may as well get one ... |
21-2-2013 at 05:53 by: kadriver |
Digital pH meters for sale Doc B
I use boiling oxalic acid in some of my processes.
But first I must adjust the pH to abo ... |
20-2-2013 at 10:46 by: kadriver |
Cole Parmer Lab Monitor III (discontinued) I stumbled across one of these and it was very cheap ($15 USD) so I bought it.
Trouble is, I have ... |
20-2-2013 at 09:35 by: kadriver |
Growing Microbes in a beaker Nice post, I'll google it
I agree, the quote sounds like he must have been looking through the mi ... |
20-2-2013 at 06:10 by: kadriver |
This time I'm selling it all Do you still have the Yamato rotavap glassware for sale?
kadriver |
20-2-2013 at 06:02 by: kadriver |
Growing Microbes in a beaker Hello,
Back in grade school we did a cool experiment where we put dead grass clippings in a 1 lit ... |
19-2-2013 at 21:13 by: kadriver |
Hardest Glassware to Clean Try boiling aqua regia - 4 parts concentrated (32%) hydrochloric acid and 1 part concentrated (68% t ... |
18-2-2013 at 21:33 by: kadriver |
Yamato rotavap glassware set Ephesian,
I am very much in the market for one if the price is right.
I've sent you a message ... |
18-2-2013 at 21:25 by: kadriver |
Starting a lab, striking the right balance (beginners please read). I have several test tube brushes with metal handles.
They get real rusty after a few uses.
Is ... |
18-2-2013 at 21:22 by: kadriver |
Yamato rotavap glassware set He may have what I am looking for (it is a cold trap instead of water-cooled condenser). I may have ... |
18-2-2013 at 06:50 by: kadriver |
Yamato rotavap glassware set Thanks for the guidance.
The one on eBay is for a type B vertical, I would buy it but first I mus ... |
17-2-2013 at 20:35 by: kadriver |
Yamato rotavap glassware set Also, if anyone has a partial set such as just the condenser, or just the receiver, I would be inter ... |
17-2-2013 at 11:29 by: kadriver |
Stainless Steel Bowl as the Cathode [rquote=275094&tid=23390&author=KonkreteRocketry]Any one knows if pencil lead can be used in ... |
17-2-2013 at 10:44 by: kadriver |
Stainless Steel Bowl as the Cathode [rquote=275073&tid=23390&author=cyanureeves]would this work with silver coins composed of 80 ... |
17-2-2013 at 10:36 by: kadriver |
Stainless Steel Bowl as the Cathode [rquote=274982&tid=23390&author=DONALD W]Nice set-up.
Where did you get your variable powe ... |
17-2-2013 at 10:09 by: kadriver |
Stainless Steel Bowl as the Cathode I modified my electrolytic silver cell to use a non-magnetic stainless steel bowl as the cathode for ... |
16-2-2013 at 06:23 by: kadriver |
Sodium Bromate Thanks woelen.
I will do the dilute sulfuric acid test on the bromate that I aquired to see if I ... |
16-2-2013 at 05:27 by: kadriver |
What chemicals do you need? I bought two hard to get chemicals from Ephesian on Tuesday and they arrived on Thursday.
The pri ... |
15-2-2013 at 10:40 by: kadriver |
Electrolytic Silver Cell Hello:
Both Fleaker and Intergalactic_Captain are way over my head with respect to the chemistry. ... |
14-2-2013 at 21:41 by: kadriver |
Sodium Bromate Is there another solvent (other than water) that can be used to separate the bromate from the bromid ... |
12-2-2013 at 00:04 by: kadriver |
Pyrex gas washing bottle I love mine, I have 2 - a 500ml and a 250ml
look at this post and you will see a video of my expe ... |
1-2-2013 at 21:57 by: kadriver |
Clean Sulfur Dioxide Gas As promised, here is the video showing the use of SO2 gas to precipitate gold from a gold chloride s ... |
1-2-2013 at 21:43 by: kadriver |
Clean Sulfur Dioxide Gas woelen, I agree with you. The dilute H2SO4 dripped on the dry Na2S2O5 seems less messy. I do plan to ... |
1-2-2013 at 06:27 by: kadriver |
Clean Sulfur Dioxide Gas Here is a great article on the apparatus and chemicals needed to make SO2.
The article says that ... |
31-1-2013 at 21:13 by: kadriver |
Clean Sulfur Dioxide Gas I granulated the 16 gram gold button this evening.