Search |
[Next Page] |
Platinum plated titanium profit?
the market price of one gram of Pt is 45$ so no profit there.
and IIRC you dont need a lo ... |
6-11-2007 at 05:55 by: hashashan |
Platinum plated titanium 60 bucks for that crap? i bet it doesnt contain even 1 gram of Pt.
why wont you just make it yours ... |
6-11-2007 at 04:39 by: hashashan |
More on PbO2 electrodes Well guys I think I have an update.
Recently I was working on a massive anode.
The anode was grow ... |
5-11-2007 at 23:56 by: hashashan |
More on PbO2 electrodes But wont such beads flying around in the solution with enough speed to knock off the bubbles hurt my ... |
17-10-2007 at 08:24 by: hashashan |
More on PbO2 electrodes Glass what? what are those? |
17-10-2007 at 07:38 by: hashashan |
More on PbO2 electrodes Experimentation is nice and all, but only untill it is getting close to lead salt spills. |
16-10-2007 at 23:50 by: hashashan |
More on PbO2 electrodes So if there will be foaming, whats wrong with just soap? |
16-10-2007 at 14:37 by: hashashan |
More on PbO2 electrodes Ill try to find those where I live. |
16-10-2007 at 00:08 by: hashashan |
More on PbO2 electrodes I may obtain them but i have no idea where do you get them guys. Ant chance that they will be in a c ... |
14-10-2007 at 01:45 by: hashashan |
More on PbO2 electrodes I already discussed the silver issue with dann and explained to him that because both silver chlorat ... |
13-10-2007 at 06:24 by: hashashan |
More on PbO2 electrodes Update : Installed the anode in a NaClO3 cell. It works, but it seems like most of my silver pits we ... |
12-10-2007 at 08:49 by: hashashan |
More on PbO2 electrodes Well guys I think i've hit the jackpot. Still not sure though.
I took a piece of Ti, made some pit ... |
11-10-2007 at 15:51 by: hashashan |
More on PbO2 electrodes The iron wasn't a substrate, It was later removed exposing a massive 5-7mm anode.
The cell was PH ... |
7-10-2007 at 04:55 by: hashashan |
More on PbO2 electrodes [quote][i]Originally posted by dann2[/i]
[quote][i]Originally posted by hashashan[/i]
Hi, did some ... |
6-10-2007 at 21:29 by: hashashan |
Scrounging for mercury You can always buy thermometers |
1-10-2007 at 00:08 by: hashashan |
More on PbO2 electrodes Hi, did some alpha lead plating, weired thing... i only got a thin brown plating, couldnt get the th ... |
1-10-2007 at 00:01 by: hashashan |
More on PbO2 electrodes Never seen it here. |
26-9-2007 at 09:26 by: hashashan |
More on PbO2 electrodes Sorry for reviving a dying thread,
Anyone knows any way to make an alpha lead dioxide coating? I d ... |
26-9-2007 at 05:54 by: hashashan |
Flash Powder How about steel media? |
17-9-2007 at 23:34 by: hashashan |
Sodium chlorate cells Once again I don't really understand. Your cell never has 100% chlorate in it ... Id suppose it has ... |
17-9-2007 at 12:35 by: hashashan |
Sodium chlorate cells How do you know its the chlorate crystalizes out and not the Chloride? |
17-9-2007 at 03:59 by: hashashan |
Sodium chlorate cells [quote][i]Originally posted by 209[/i]
And I guess I sodium chlorate should start forming on the bo ... |
16-9-2007 at 14:13 by: hashashan |
Flash Powder Al is problematic gor me ... I can get only 325 granular Al here (the dark i should make myslef and ... |
4-9-2007 at 22:46 by: hashashan |
Flash Powder I prefer to use Mg flashes, they are much more powerfull then Al |
3-9-2007 at 21:53 by: hashashan |
Phenol from Light Sticks Just read the thread about the so called "glowing tomatoe" and one of the links caught my interest. ... |