Search |
[Next Page] |
Lithium hydride Well, some used hydrogen generated from LiH, but CaH2 probably does a better job, and it is easier t ... |
19-12-2015 at 17:21 by: zed |
Platinum for catalyst - what's best shape/formation? Ummmm. I don't know much, but in liquid phase hydrogenations, Platinum Catalysts, are usually produ ... |
17-12-2015 at 17:36 by: zed |
Is 4-ethylphenyl-2-nitropropene liquid in room temperature? Once again, this is not a very healthy pursuit, especially for a chemist. Having an unlimited supp ... |
15-12-2015 at 18:05 by: zed |
Plating cadmium or chromium onto iron? Well, yeah. You could Blue it. As in gun bluing. Or, you could coat it with vegetable oil, and c ... |
7-12-2015 at 19:35 by: zed |
Diethylamine Hydrochloride Synthesis Hmmm. Perhaps, the list has changed.
Seems like I remember Diethylamine as being listed.
Ther ... |
1-12-2015 at 17:03 by: zed |
methyl methacrylate How did you polymerize the material. Also, how serious a lachrymator is this stuff?
One equals ... |
29-11-2015 at 16:53 by: zed |
Paint creation thread https://en.wikipedia.org/wiki/Cobalt_phosphate
Cobalt Violet, interesting color.
The eye may b ... |
27-11-2015 at 17:43 by: zed |
methyl methacrylate Ummm. Alkylations of the Indole 3 position, via refluxing Indole with Acetic Anhydride, and materia ... |
24-11-2015 at 18:35 by: zed |
Is 4-ethylphenyl-2-nitropropene liquid in room temperature? Well, this ain't exactly a healthy pursuit.
That being said, the standard crystallization method, ... |
24-11-2015 at 18:05 by: zed |
Paint creation thread "No problem buying poppy seeds for use in cooking, the art supply store in town sells refined poppy ... |
23-11-2015 at 16:39 by: zed |
Nitromethane, nitroethane, nitropropane synthesis via industrial route Ummmm, well. Most of you seem to be intent on "cracking" propane. It isn't the best approach.
T ... |
19-11-2015 at 16:29 by: zed |
Paint creation thread
"Do you know of any other oils that polymerizes in the presence of air like linseed oil? It's hard ... |
19-11-2015 at 15:52 by: zed |
methyl methacrylate Methyl Methacrylate is an interesting reagent. I don't need it, but somebody might.
I had a Kilo ... |
17-11-2015 at 18:26 by: zed |
Stainless Steel resistance to acids There are "Stainless Steels" that have pretty good acid resistance. Only problem is, the best of th ... |
17-11-2015 at 18:08 by: zed |
Is 4-ethylphenyl-2-nitropropene liquid in room temperature? Some sort of Dean Stark setup isn't hard to construct, and in a pinch, simple distillation might do. ... |
12-11-2015 at 15:05 by: zed |
Diamond synthesis Seen quite a few Synthetic Stones. The tastiest of them all, was the Gilson Emerald. Not Cheap in ... |
11-11-2015 at 15:17 by: zed |
Obtaining chemicals Oz can be very unfriendly, to chemical curiosity.
That being said, you can generally find somebod ... |
10-11-2015 at 15:10 by: zed |
"Hacked/Modified" Microwave to 2-3x power (4,000 watts) - thoughts? The question is..."Do you need all of that power, for some special reason?"
Many people have repo ... |
10-11-2015 at 14:58 by: zed |
Diamond synthesis Yeah, in my estimation, current Gold prices are the result of speculation (or loss prevention).
G ... |
10-11-2015 at 14:21 by: zed |
megalomanias Site Bad intent? We are deluged by folks with bad intent. Leastwise, we assume they have bad intent.
... |
10-11-2015 at 14:01 by: zed |
Diamond synthesis There is no real shortage of Diamonds. Global output is carefully controlled, by the folks at DeBee ... |
9-11-2015 at 15:15 by: zed |
Paint creation thread There are books on this topic. I have an interest myself, because oil based house paints are no lon ... |
9-11-2015 at 14:52 by: zed |
Constructing a vacuum chamber
"It just seemed like a hassle to try and deal with a pressure cooker, since they have 2 layers of ... |
8-11-2015 at 14:23 by: zed |
On treasure hunt - not lucky this time Mouse-brain?
|
7-11-2015 at 13:17 by: zed |
Water Aspirator Help Hmmm. What is your rate of flow like?
Personally, I come from a less eco-friendly generation. ... |
7-11-2015 at 13:03 by: zed |
[Next Page] |