Flash Powder Dark aluminum, simply put, is not prepared by just ball milling it. Dark Aluminum has some carbon a ... |
18-9-2007 at 21:45 by: Mumbles |
Identification of Protein We went over the process the other day in biochem, I can post some truncated notes if you'd like. A ... |
18-9-2007 at 07:49 by: Mumbles |
Flash Powder I'd suggest going and doing some reading about the processes that go into manufacturing dark aluminu ... |
18-9-2007 at 07:46 by: Mumbles |
Identification of Protein I believe most of the containers just say "Whey Protein concentrate". Something like this is fairly ... |
17-9-2007 at 21:48 by: Mumbles |
Flash Powder I do believe you will encounter some relative difficulty preparing your own dark aluminum. Believe ... |
17-9-2007 at 21:40 by: Mumbles |
Peroxide Safety Maybe.
The mechanism by which it removes the peroxide is to reduce the bond. It reduces the pero ... |
24-5-2007 at 13:26 by: Mumbles |
mercury Mercury as vapor is where it gets dicey though.
A school around me had a mercury spill a few ye ... |
23-5-2007 at 09:02 by: Mumbles |
Oxygen Production with H2O2 I seem to remember I2 or KI working as well. I'm sure you could find iron oxide around somewhere. ... |
22-5-2007 at 13:15 by: Mumbles |
Sodium Nitrate production I've been away a long time. Would you mind pointing me in the direction of the dilute HNO3 from AN ... |
22-5-2007 at 13:06 by: Mumbles |
Concentrating Vinegar If you have the equipment to distill, thing may be a lot faster and easier for you. Neutralization ... |
20-5-2007 at 20:38 by: Mumbles |
Dear god... I have a LOT of sodium metal. For my sorta AP chem class we had a professor who did some demos I really doubt he was supposed to d ... |
21-4-2007 at 22:41 by: Mumbles |
What’s the average age? I've also changed demographics since I voted. Hit the big 2-0 a few months ago(Don't tell the liquo ... |
10-4-2007 at 16:55 by: Mumbles |
synthesizing copper benzoate? It's hard to tell exactly what it was. All the symptoms are relatively similar as far as what I exp ... |
28-3-2007 at 10:52 by: Mumbles |
synthesizing copper benzoate? The poisoning lifted after about 24 hours. Now I just have some lung irritation and a cough. It al ... |
27-3-2007 at 18:36 by: Mumbles |
synthesizing copper benzoate? No, no masses were taken, short of the initial amounts of copper sulfate and sodium benzoate. It wa ... |
26-3-2007 at 08:20 by: Mumbles |
synthesizing copper benzoate? I had a go at preparing some copper benzoate today. I wasn't looking for yield, just properties. I ... |
25-3-2007 at 13:27 by: Mumbles |
Phosphine and white P from sodium hypophosphite? I do believe sodium hypophosphite is the secret ingredient to super black, supposedly the blackest b ... |
24-3-2007 at 23:23 by: Mumbles |
nichrome in solution.. In a solution addition of iron will precipitate the nickel but not the chromium. I'd add some NaOH ... |
24-3-2007 at 10:08 by: Mumbles |
How Did You get Started in Chemistry? I have to admit, reading this thread makes me all warm and fuzzy inside thinking about how I got sta ... |
23-3-2007 at 20:19 by: Mumbles |
Mortar and pestle, and others Look around for home school suppliers. They will be able to provide you with many basic science sup ... |
28-2-2007 at 21:25 by: Mumbles |
Suggest some experiments If you're interested in straight chemistry, I'd suggest picking up a copy of Vogel's Practical Organ ... |
26-2-2007 at 19:45 by: Mumbles |
Books threads are moving to dedicated forum I just wasn't sure how many people would remember me. I'm sure if anyone in power had doubts I coul ... |
26-2-2007 at 19:17 by: Mumbles |
Books threads are moving to dedicated forum Nice to see all you guys again.
I was just wondering if there was an idleness clause is this. I ... |
26-2-2007 at 15:20 by: Mumbles |
colorfast black dye for cotton I've only been able to get brown from permanganate, though never intentionally. I want to say iodin ... |
24-2-2007 at 22:20 by: Mumbles |
Red Flash Powder Yes, but adding a few percent boric acid will effectivly kill the reaction. I had some complex vers ... |
11-7-2006 at 18:17 by: Mumbles |