Search |
[Next Page] |
Reducing sodium molybdate by nascent hydrogen http://svetprvku.cz/12-prvky
Molybden - prášek
Čistota 99,9%
6 CZK (0,25 EUR) per 1 g
49 g in ... |
22-2-2020 at 00:06 by: Fery |
Azelaic acid saponification:
102,5 g SOHO + 25,2 g 85% KOH + 100 ml 95% C2H5OH
[file]79480[/file] [file]7948 ... |
21-2-2020 at 11:53 by: Fery |
azelaic acid - most efficient method related to KMnO4 This experiment focused on squeezing KMnO4 as much as possible:
Oxidation was performed in 3 steps ... |
21-2-2020 at 10:14 by: Fery |
ethyl hexanoate - pineapple ester 65% yield (0,53 mol) calculated from the amount of hexanoic acid (0,81 mol)
ethanol added in 3-fold ... |
21-2-2020 at 00:40 by: Fery |
ethyl hexanoate - pineapple ester this ester has more pleasant scent than [url=https://www.sciencemadness.org/whisper/viewthread.php?t ... |
20-2-2020 at 09:47 by: Fery |
ethyl butyrate - pineapple ester I wanted to preform this synthesis decades ago but it was postponed till today, when my dream came t ... |
19-2-2020 at 10:02 by: Fery |
HCl gas generator for making (NH4)2[MoOCl5] Those at room temperature - dehydrating 37% HCl using CaCl2 you mentioned or conc. H2SO4 works too. ... |
19-2-2020 at 05:19 by: Fery |
ISO Terbium https://onyxmet.com/index.php?route=product/product&product_id=2715%22
46 EUR / 10 g |
19-2-2020 at 00:22 by: Fery |
Allyl Bromide Preparation reactants
[file]79416[/file]
apparatus - !!! note the hose from the vacuum take-off adapt ... |
18-2-2020 at 04:04 by: Fery |
allyl alcohol preparation from glycerol + formic acid Be very careful - allyl alcohol has significantly higher toxicity (pls read the pdf attached) than o ... |
18-2-2020 at 03:22 by: Fery |
Sodium permanganate anti - what's a pity, here you could just enter the pharmacy and tell something like: I have a mycot ... |
18-2-2020 at 02:49 by: Fery |
Allyl Bromide Preparation I would like to write my own opinion.
The inert gas is probably unnecessary. Seems water steam expe ... |
17-2-2020 at 12:58 by: Fery |
dissolving W in H2O2 Hi sbreheny, this is without thorium, the green color means pure 99,8% W.
I have also about half a ... |
17-2-2020 at 12:47 by: Fery |
Sodium permanganate Maybe you can buy small amount like 20 g of KMnO4 in pharmacy. It is used to treat mycotic infection ... |
17-2-2020 at 12:35 by: Fery |
dissolving W in H2O2 Here my experiment - dissolving tungsten in hydrogen peroxide. Unfortunately there is no info about ... |
16-2-2020 at 04:14 by: Fery |
Tungsten compound [rquote=541850&tid=96118&author=woelen]Pure tungsten dissolves in 10% H2O2 fairly easily, no ... |
16-2-2020 at 03:12 by: Fery |
Tungsten metal plus piranha solution? I've just finished some experiments and my opinion is that ammonia speeds up H2O2 decomposition.
Yo ... |
16-2-2020 at 02:55 by: Fery |
Ni(IV) - periodatonickelates woelen and Tdep, if you are interested in NaBrO[sub]4[/sub] then it is easier to separate it when re ... |
11-2-2020 at 03:52 by: Fery |
photos reactants - KIO4, NiSO4 . 6 H2O, K2S2O8
[file]79250[/file]
3,0 g KIO4 + 500 ml H2O + 2,0 ... |
10-2-2020 at 08:57 by: Fery |
Ni(IV) - periodatonickelates KNiIO6 . 1/2 H2O
Dissolve 3,0 g KIO4 in 500 ml boiling water in 1 l Erlenmayer flask, then add 2,0 ... |
10-2-2020 at 08:42 by: Fery |
photos 48% HBr + 0,10 g CuO
[file]79158[/file] [file]79160[/file]
after adding 1,00 g CuO totall ... |
7-2-2020 at 08:25 by: Fery |
KBr.CuBr2 double salt aka KCuBr3 I found this info about 1 year ago:
http://copper.atomistry.com/cupric_bromide.html
[quote]double ... |
7-2-2020 at 08:09 by: Fery |
anomalies in chemistry Please post here anomalies in chemistry.
Searching the forum, I found only this one post concerin ... |
7-2-2020 at 04:55 by: Fery |
Divalent chromium Hi Bedlasky here a small gift for you. I did the synthesis a long long long ago (prep for IChO).
Ev ... |
7-2-2020 at 03:04 by: Fery |
Red Phosphorus Source back to the topic - I have to recommend onyxmet.com
courier delivered my parcel the 4th day (it cou ... |
7-2-2020 at 02:12 by: Fery |