Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Um, if you mean my persistence, then I agree; but I really only have an undergraduate course in inor ... |
23-11-2023 at 15:53 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Unusually nice.
This morning, all solds were dissolved. Centerfuging, not needed.
From the di ... |
23-11-2023 at 08:41 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Today's experiment, #490
I've got some plating activity on the higher current electrode.
Not sur ... |
22-11-2023 at 22:49 by: semiconductive |
Using Corning PC-425D on 240V After looking at the pictures, I'm going to say the answer is NO. You will have trouble using this ... |
22-11-2023 at 14:17 by: semiconductive |
Using Corning PC-425D on 240V [rquote=688793&tid=159982&author=print118]I made an error with the model, my apologies. The ... |
22-11-2023 at 13:59 by: semiconductive |
Laboratory power supply constant current How constant of a current do you want?
A light bulb filament happens to be a decent current regul ... |
21-11-2023 at 23:36 by: semiconductive |
What happens to capacities of batteries when connected in series or parallel? [rquote=373209&tid=44458&author=unionised][rquote=363242&tid=44458&author=franklyn]S ... |
21-11-2023 at 23:26 by: semiconductive |
Using Corning PC-425D on 240V I don't have one to check.
But: I know that the 240V corning plate and 120V corning plate have th ... |
21-11-2023 at 23:03 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. All comments, welcome; Thanks!
Anode material, pure nickel wire, 0.9mm diameter, spooled around 6 ... |
21-11-2023 at 18:32 by: semiconductive |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. I've been experimenting for around two years with electroplating of metals in orgainc liquids. I've ... |
19-11-2023 at 15:09 by: semiconductive |
Questions in electroplating I'm less knowledgeable than others here; I've been experimenting with waterless plating of iron for ... |
19-11-2023 at 14:32 by: semiconductive |
methanol/ionic liquid electroplaing of metals [rquote=659572&tid=157386&author=clearly_not_atara]pKa H2O: 15.7
pKa MeOH: 15.5
Methanol ... |
26-2-2023 at 20:02 by: semiconductive |
methanol/ionic liquid electroplaing of metals It's been over a year, and around 360 different experiments.
Most alcohol baths, seem to be entropy ... |
26-2-2023 at 16:29 by: semiconductive |
de-aromatization and removal of ethene bonds. Thank you for the link.
I'll continue to study it for a week more, before becoming annoyed. But ... |
19-11-2022 at 23:31 by: semiconductive |
ZnCl2 * nH2O, purificiation My beginner luck.
From 107C yesterday, all the way to 125C this morning ... and it still didn ... |
19-11-2022 at 21:35 by: semiconductive |
ZnCl2 * nH2O, purificiation It is indeed *more concentrated* Hcl in the trap than in the bottle below it.
Density is 2% higher ... |
18-11-2022 at 14:18 by: semiconductive |
de-aromatization and removal of ethene bonds. Not alpha pinine to OL, I just managed to make synthetic amber. It's rock hard.
|
18-11-2022 at 13:20 by: semiconductive |
de-aromatization and removal of ethene bonds. Totally fair. ![:)](./images/smilies/smile.gif)
I am an Electrical Engineer, so I've only had inorganic chemistry.
I bought pal ... |
18-11-2022 at 12:43 by: semiconductive |
de-aromatization and removal of ethene bonds. I'm just curious. ( Beginner question. )
There are a lot of essential oils from 'green' sources ... |
17-11-2022 at 23:50 by: semiconductive |
ZnCl2 * nH2O, purificiation First distill test:
12 hours at 95C.
A few drops distilled over, maybe 2CC out of 100. There has ... |
17-11-2022 at 13:36 by: semiconductive |
ZnCl2 * nH2O, purificiation [quote]
Preparation of anhydrous methanolic HCl likely requires gassing.
[/quote]
This goes bac ... |
17-11-2022 at 11:01 by: semiconductive |
ZnCl2 * nH2O, purificiation [rquote=678354&tid=158980&author=teodor]
So, the ZnCl2 * HCl * 2H2O adduct loses HCl tog ... |
16-11-2022 at 13:00 by: semiconductive |
ZnCl2 * nH2O, purificiation I realize there is a difference between dry and anhydrous.
I'm just noticing with regular salt, tha ... |
3-11-2022 at 22:52 by: semiconductive |
ZnCl2 * nH2O, purificiation Azetropic HCl ought to boil off uniformly by itself, and come back with the same concentration after ... |
2-11-2022 at 22:30 by: semiconductive |
ZnCl2 * nH2O, purificiation Thanks for the input.
I thought about this, and tried an acetone process first just to experiment ... |