Search |
[Next Page] |
Antimony analog of Paris Green? Copper chlorate, as I recall, is indeed explosive, but also highly hygroscopic. A primary explosive ... |
24-3-2009 at 07:13 by: Mumbles |
What ELSE is in the sulfur? It's common for the 10% to be a clay for the reasons already stated. Separation can be as easy as a ... |
3-12-2008 at 18:30 by: Mumbles |
Vacuum grease substitute? It seems that mixing the starch and the glycerol at elevated temperature is designed to covert starc ... |
22-5-2008 at 18:48 by: Mumbles |
destroying chlorates and leaving the prechlorates Yes, you will likely need acid to reduce it via ferrous sulfate. I've always thought of it somethin ... |
26-2-2008 at 12:41 by: Mumbles |
cheap zeolites They're not the best price, but still not extremely bad for the small quantity. I have about 5lbs o ... |
26-2-2008 at 12:25 by: Mumbles |
Latest chemical order? Mine isn't nearly as chemically exciting as most of your guys'. I got a 55lb bag of soluble glutono ... |
16-2-2008 at 20:05 by: Mumbles |
stupid still or probably the user One simple fix would be to wrap the distillation adapter in aluminum foil or something similar. It ... |
27-1-2008 at 23:26 by: Mumbles |
Teach `em Young! I, as some others, am lacking in children and wives. Not quite my thing just yet, perhaps in 10 yea ... |
16-1-2008 at 14:11 by: Mumbles |
powdered Zn I believe the normal ratios are normally quite close to stoichiometric. My notes show a ratio of 67 ... |
6-1-2008 at 22:26 by: Mumbles |
potassium nitrate burning realy slow I've honestly heard conflicting reports about activated. Some say yey, while some say ney. Probabl ... |
6-1-2008 at 22:20 by: Mumbles |
Magnesium I knew the owners of magnesiumsales sort of well. They used to be somewhat frequent posters on APC. ... |
6-1-2008 at 16:21 by: Mumbles |
potassium nitrate burning realy slow Spreading the granulated product on a few sheets of news paper will have it dry pretty quickly. Sti ... |
2-1-2008 at 22:50 by: Mumbles |
potassium nitrate burning realy slow Indeed I am. Given my status there, I unfortunatly do not get to visit here as much as I would like ... |
2-1-2008 at 20:20 by: Mumbles |
Wine recommendations? Last year I took it upon myself to make some mead in honor of my viking heritage. One turned out we ... |
2-1-2008 at 20:08 by: Mumbles |
potassium nitrate burning realy slow The charcoal has easily the largest impact upon the speed of the charcoal. However, it is your meth ... |
2-1-2008 at 19:50 by: Mumbles |
decompostion of sulfurous acid I've heard the same thing about the heating in a glass tube producing solid sulfur. I could have sw ... |
2-1-2008 at 19:09 by: Mumbles |
Pyrotechnic Mixtures I appreciate the kind words about my forum. It's always nice to hear my years of work there were no ... |
28-12-2007 at 22:03 by: Mumbles |
HEET as a source for methanol Back a few years ago I distilled some Heet for methanol. It came over just fine. As with anything ... |
12-11-2007 at 21:59 by: Mumbles |
Good book on bonding theory? We've been learning some more advanced bonding theory in my Inorganic Chem class from a symetry pers ... |
29-10-2007 at 23:05 by: Mumbles |
N-azides (azidamines) And the second article you requested. This one is much more promising if I do say so myself.
I'm ... |
29-10-2007 at 22:40 by: Mumbles |
separating Toluene from the azeotrope with Ethanol Just out of curiosity, but do you desire both compounds back, or just the toluene? The thought of a ... |
29-10-2007 at 22:27 by: Mumbles |
what did i make? Cu+H20+NaCl+NaOH-=? It can be found in larger quantities and cheaper as some sort of pond additive. I believe it either ... |
28-10-2007 at 15:33 by: Mumbles |
N-azides (azidamines) The journal you expressed interest in is attached. They use tosyl azide as the agent, and run the r ... |
28-10-2007 at 13:08 by: Mumbles |
Exotic thermites & analogs I've always found thermite to rarely live up to the legend of burning through engine blocks and all ... |
19-9-2007 at 20:53 by: Mumbles |
Flash Powder He was discussing flash, and that generally makes me automatically go to the blackhead types. A dar ... |
19-9-2007 at 09:48 by: Mumbles |