Balanced equation makes no sense I have been making copper nitrate using this stoichiometry many times and never questioned it:
Cu + ... |
14-1-2015 at 00:53 by: CHRIS25 |
Best Acid that will get rid of rust quickest without harming iron? [rquote=387274&tid=61152&author=WGTR] If you use hydrochloric acid, after rinsing the acid ... |
13-1-2015 at 01:21 by: CHRIS25 |
Best Acid that will get rid of rust quickest without harming iron? I have used HCl on steel and it worked beautifully, about a 6M solution on a heavily rusted replica ... |
12-1-2015 at 09:17 by: CHRIS25 |
A first step towards the staircase.. @Bert ...And a Very Important Announcement from the Department of Health and Human Services!!!....
... |
11-1-2015 at 23:34 by: CHRIS25 |
Ferrofluid-Art Allow me to say that the following is in a friendly tone My divergence from your
stance is only o ... |
10-1-2015 at 02:59 by: CHRIS25 |
Ferrofluid-Art Gamma, if you understood the meaning of this word you would not have said ===Psssst, PNG has gamma. ... |
9-1-2015 at 01:44 by: CHRIS25 |
Ferrofluid-Art [rquote=386377&tid=60661&author=Etaoin Shrdlu][rquote=386229&tid=60661&author=CHRIS2 ... |
7-1-2015 at 07:47 by: CHRIS25 |
Sodium Silicates I need to do some titrations with silicates. One of my silicates is unidentifiable with respect to ... |
7-1-2015 at 03:33 by: CHRIS25 |
Ferrofluid-Art [rquote=386144&tid=60661&author=BJ68]Part 2:
I made the error to save the image file as JPG ... |
7-1-2015 at 00:22 by: CHRIS25 |
Copper carbonate - controlling the colour [b]Update[/b]
Posting an image of the reaction, this was started on 1 january, and by day 2 the m ... |
6-1-2015 at 09:50 by: CHRIS25 |
Amygdalin from Apple Seeds [ EXPERIMENTS AND RESULTS] Not that I would ever touch anything like this - but to avoid chemicals and experimentation with suc ... |
3-1-2015 at 03:00 by: CHRIS25 |
Copper carbonate - controlling the colour [rquote=384714&tid=50822&author=blogfast25]Your point about the limestone containing 78.9 % ... |
2-1-2015 at 11:03 by: CHRIS25 |
Copper carbonate - controlling the colour [rquote=384689&tid=50822&author=blogfast25]Chris, have a look at this.
Scroll down to abo ... |
2-1-2015 at 08:51 by: CHRIS25 |
Copper carbonate - controlling the colour @Blogfast - See it, got it. Why on earth I did that ?
@Aga - Corn starch. It worked for titrating ... |
1-1-2015 at 11:47 by: CHRIS25 |
Copper carbonate - controlling the colour Yes absolutely - what you said is what I measured exactly, once again it is my Maths to be blame, an ... |
31-12-2014 at 09:33 by: CHRIS25 |
Quartz Pebbles Greatly appreciated, will get onto this in the coming days. And thanks for the density link. |
31-12-2014 at 09:18 by: CHRIS25 |
Copper carbonate - controlling the colour I'll keep this short. After 8 titrations over two weeks and two today I can safely say this: Corn s ... |
31-12-2014 at 08:48 by: CHRIS25 |
Quartz Pebbles Well as for hardness, there were no visible scratch marks after scraping with iron or titanium metal ... |
31-12-2014 at 08:12 by: CHRIS25 |
Quartz Pebbles Ah such a shame then. There are so many different types of rocks here to see, every single beech, o ... |
31-12-2014 at 01:43 by: CHRIS25 |
Quartz Pebbles Not being familiar at all with Geology I wanted to identify these pebbles, after some searching I pr ... |
30-12-2014 at 12:30 by: CHRIS25 |
Problem with the "sup" button For some reason the 'sup' button no longer works. I have tried the 'sub' and 'sup' buttons many man ... |
30-12-2014 at 00:11 by: CHRIS25 |
Copper nitrates Yes I agree I should have written the formula you wrote this is what I meant actually. I have separa ... |
29-12-2014 at 11:59 by: CHRIS25 |
Copper nitrates Excuse the interjection, but since anhydrous copper nitrate was mentioned I thought I would post thi ... |
29-12-2014 at 11:02 by: CHRIS25 |
Copper nitrates I would use 50% without doubt. Conc nitric is 16 M roughly, I just used an 8 M on 32 g of cleaned c ... |
29-12-2014 at 09:22 by: CHRIS25 |
Copper nitrates I suspect, and bravely so I might add, that the green is copper sulphate. Cu3(SO4)(OH)4. Personall ... |