Sodium Garbage Time And Unusual Results Blog, 'block' is a generic term I use for the solidified melt. I use an iron vessel for the crucible ... |
25-4-2011 at 10:57 by: m1tanker78 |
Make Potassium (from versuchschemie.de) Blogfast, you're bringing a [cheerful] tear to my eye. First, you broke from convention and did the ... |
25-4-2011 at 10:49 by: m1tanker78 |
Sodium Garbage Time And Unusual Results First, let me explain what 'garbage time' or 'trash time' is. I normally reuse the electrolysis bloc ... |
25-4-2011 at 09:31 by: m1tanker78 |
calcium chloride from calcium carbonate (using a chloride salt) Why not run chlorine from your generator through a column of hydrated lime? Lime is excruciatingly c ... |
25-4-2011 at 07:49 by: m1tanker78 |
Pretty Pictures (1) Macro shots with a [i]cell phone...[/i]
Unknown carbon compound that begins life as glossy planar ... |
22-4-2011 at 16:05 by: m1tanker78 |
Sodium - Random Crystal Arrangement Thanks for the link mr. crow. That's exactly what I was looking for.
Tom |
22-4-2011 at 11:40 by: m1tanker78 |
Sodium - Random Crystal Arrangement Hopefully someone can help me out with this:
I cut a piece of sodium metal, let it oxidize in air ... |
21-4-2011 at 18:56 by: m1tanker78 |
Plating? Cheapest, safest demonstration? You can't go wrong with a copper plating on a quarter demo. You'll obviously need to use HCl but is ... |
19-4-2011 at 12:19 by: m1tanker78 |
Pretty Pictures (1) [rquote=207291&tid=14644&author=bfesser]Mg is exceedingly cheap and easy to come by. 10% Na ... |
19-4-2011 at 11:25 by: m1tanker78 |
Sodium by electrolysis? I also think your choice of salt is BAD but I have a couple of questions for you, JCM.
1. What ma ... |
19-4-2011 at 06:09 by: m1tanker78 |
Pretty Pictures (1) Don't judge a book by its cover?
Unrefined sodium nugget dissected to check internal integrity ... |
18-4-2011 at 13:43 by: m1tanker78 |
Experiments?? Yeah, you need some garage time!
[quote]I am also looking for some cool easy experiments to sh ... |
16-4-2011 at 15:43 by: m1tanker78 |
Make Potassium (from versuchschemie.de) BlogFast: I don't mean to be a pest but can you describe the black stuff in a little more detai? You ... |
15-4-2011 at 13:59 by: m1tanker78 |
stannous chloride Could be copper. This happened to me a few days ago (although it was an experiment aimed at making q ... |
13-4-2011 at 12:35 by: m1tanker78 |
Iron Oxide question Robert, I may have missed something but you want ferric chloride to etch PCB's? If you use the toner ... |
10-4-2011 at 06:57 by: m1tanker78 |
Make Potassium (from versuchschemie.de) [rquote=206369&tid=14970&author=blogfast25]Nice balls of sodium, tanker78!
Have you seen ... |
9-4-2011 at 19:21 by: m1tanker78 |
Make Potassium (from versuchschemie.de) @BlogFast: Holy frijolee! Awesome experiment! I admit that I skipped over the entire thread but I'll ... |
9-4-2011 at 07:32 by: m1tanker78 |
sand filter help please It depends on what you plan to run through it. For general use here's what I do...
Run it through ... |
8-4-2011 at 18:32 by: m1tanker78 |
Stannous Chloride - An Idea [quote] As for potassium, I'm really eager to get my order of KOH and try ot the cool german experim ... |
8-4-2011 at 16:06 by: m1tanker78 |
Stannous Chloride - An Idea [rquote=205793&tid=15932&author=Arthur Dent]
As much as I am starting to have a pretty dece ... |
8-4-2011 at 12:40 by: m1tanker78 |
Got Juiced By an Microwave oven transformer [quote]DO I need to go in and get checked out?[/quote]
Make an appointment with the hairdresser? ... |
6-4-2011 at 19:36 by: m1tanker78 |
Stannous Chloride - An Idea Robert, I'm a little envious of your tin chloride (for good reason)!
The crystals in my above pic ... |
5-4-2011 at 10:07 by: m1tanker78 |
Stannous Chloride - An Idea Tin(II) chloride crystals with copper chloride impurity from the leftover solder residue:
[f ... |
5-4-2011 at 08:01 by: m1tanker78 |
ZAMAK casting alloy in HCl for Qual. Anal. exp't Going back over my notes, I see that I've gotten dark, cloudy precipitate from adding zinc (from gal ... |
4-4-2011 at 13:04 by: m1tanker78 |
ZAMAK casting alloy in HCl for Qual. Anal. exp't It's probably the aluminum content of the alloy that's giving you the dark stuff. If you want to che ... |
4-4-2011 at 11:01 by: m1tanker78 |