Peroxide Watergel I've been passed a patent # via U2U relating to H2O2 "sprengel" explosives in general, but of the ex ... |
14-1-2005 at 07:55 by: Axt |
Peroxide Watergel [quote][i]Originally posted by chemistr1[/i]
are you saying that 35% H2O2 can not be used for the s ... |
13-1-2005 at 01:00 by: Axt |
Peroxide Watergel I'm not sure if adding methanol will be useful, since to add MeOH, you decrease the concentration of ... |
12-1-2005 at 13:24 by: Axt |
Peroxide Watergel Doubling the amount of guar gum to 4% results in a more plastic mix, and holds together for longer. ... |
12-1-2005 at 07:11 by: Axt |
Peroxide Watergel Dunno, depends on the definition of "breaking power" and how well it's been interpreted into here. E ... |
12-1-2005 at 02:31 by: Axt |
Peroxide Watergel I'm not claiming a high VOD explosive, just that its a true detonation. I expect that you could ... |
10-1-2005 at 17:23 by: Axt |
Peroxide Watergel Yeh, OK. I know it <i>looks</i> like I burnt a handfull of blackpowder, but this is defi ... |
10-1-2005 at 16:27 by: Axt |
Diphoronepentaperoxide (DPPP) [quote][i]Originally posted by Joeychemist[/i]
I would not be surprised if you changed you’re tun ... |
10-1-2005 at 15:02 by: Axt |
Diphoronepentaperoxide (DPPP) [quote][i]Originally posted by Rosco Bodine[/i]
So why do you suppose what we have made is just so ... |
10-1-2005 at 14:38 by: Axt |
Peroxide Watergel The science of commercial watergel explosives is an art unto itself, where a balance of fuels (eg. A ... |
10-1-2005 at 14:15 by: Axt |
Halogenated Amines - the others Looking at both the references a few things just dont add up!
Look at the yield in the first refe ... |
10-1-2005 at 13:26 by: Axt |
Diphoronepentaperoxide (DPPP) Why not try distill the acetone/HCl mixture, and try peroxidation on both the distillate and the mot ... |
10-1-2005 at 13:12 by: Axt |
Halogenated Amines - the others I now have the original "explodes with great violence" reference. Indeed, it was heated un ... |
9-1-2005 at 04:48 by: Axt |
Exotic Primaries - Complex Salts Yes, but the ethanol should extract the bromate complex leaving the <i>sodium</i> sulpha ... |
5-1-2005 at 20:07 by: Axt |
Diphoronepentaperoxide (DPPP) Do you have a density yet Pyroz? or at least a relative density to AP? |
4-1-2005 at 23:20 by: Axt |
Any explosives made with Napthalene? View Attachment.
Naphthalene diozonide seems like one of the more isolatable explosive ozonides, ... |
4-1-2005 at 12:54 by: Axt |
Halogenated Amines - the others Anyway, 9ml of this yellow oil was compared to (true) PLX, charges were in plastic vials, taped onto ... |
3-1-2005 at 16:10 by: Axt |
Exotic Primaries - Complex Salts I dont have the amounts used anymore, I think I simply mixed the stoichiometric quantities to see if ... |
3-1-2005 at 15:37 by: Axt |
NO2 + alkene ? I've uploaded references refering to NO2 reactions <a href=http://rogue.altlist.com/banners/ ... |
3-1-2005 at 11:23 by: Axt |
Diphoronepentaperoxide (DPPP) [quote][i]Originally posted by Matsumoto_Hideki[/i]
test against 4mm steel.
[/quote]
Did you ac ... |
1-1-2005 at 22:02 by: Axt |
Had an acciedent....... Heh...
Heres some gems I found using a totally unrelated search on google.
Heres a variation o ... |
22-12-2004 at 02:36 by: Axt |
Diphoronepentaperoxide (DPPP) This isn't even up for debate. Do I really have to explain why you cant have a bonfire 3' ... |
22-12-2004 at 00:12 by: Axt |
Diphoronepentaperoxide (DPPP) We are sick of your bullshit.
Lets see what you have said so far in your short history here, and ... |
21-12-2004 at 22:17 by: Axt |
Methyl Ethyl Ketone Peroxide MEKP is slightly heavier then water, thus will sink in it, but because of MEK contaminants and the s ... |
19-12-2004 at 00:30 by: Axt |
Methylenediisonitramine I only tried once with the three metals, the copper salt yield was the smallest of the lot, even wit ... |