Can Magnesium be extracted from epsom salt easily From experience, magnesium formed by molten electrolysis is very short-lived. You'll see a bright bl ... |
4-5-2011 at 08:19 by: m1tanker78 |
Make Potassium (from versuchschemie.de) BlogFast, what did the K do in the xylene? Based on the reported densities, they should have hovered ... |
3-5-2011 at 18:21 by: m1tanker78 |
Refining Na/K From Various Processes Twospoons, I've been lurking the potassium thread, hoping someone would try this, hehe. I don't full ... |
3-5-2011 at 17:52 by: m1tanker78 |
Sodium In Naphthalene - Observations Thanks for the info kmno4. I remelted the naphthalene and dropped one of the original sodium pieces ... |
3-5-2011 at 08:12 by: m1tanker78 |
Refining Na/K From Various Processes [rquote=208780&tid=16225&author=NurdRage]
yeah... but the process is very messy since a lot ... |
3-5-2011 at 07:03 by: m1tanker78 |
Refining Na/K From Various Processes querjek, what mass?
[Edited on 5-3-2011 by m1tanker78] |
3-5-2011 at 05:36 by: m1tanker78 |
Refining Na/K From Various Processes Nurd, I assume you use the magnesiothermic reaction to yield Na? If so, what do you do with all the ... |
2-5-2011 at 18:38 by: m1tanker78 |
Synthesis of longer chain tertiary alcohols [rquote=208748&tid=15171&author=NurdRage] i've been known to be a dick.
[/rquote]
Well ... |
2-5-2011 at 17:53 by: m1tanker78 |
Refining Na/K From Various Processes I created this thread to reduce cluttering in the potassium and t-alcohol threads and to (hopefully) ... |
2-5-2011 at 17:45 by: m1tanker78 |
Synthesis of longer chain tertiary alcohols A little off topic:
NurdRage, your comment came off sounding arrogant. Don't get me wrong, I enjo ... |
2-5-2011 at 16:51 by: m1tanker78 |
Synthesis of longer chain tertiary alcohols [rquote=208674&tid=15171&author=NurdRage]no need to, i already came across using brake fluid ... |
2-5-2011 at 14:02 by: m1tanker78 |
Sodium In Naphthalene - Observations No outwardly apparent reaction. The beads formed a wrinkly dull grey skin but I believe this could h ... |
2-5-2011 at 08:54 by: m1tanker78 |
Make Potassium (from versuchschemie.de) Blog, I tried sodium in naphthalene; briefly outlined [url=https://www.sciencemadness.org/whisper/vi ... |
2-5-2011 at 07:05 by: m1tanker78 |
Sodium In Naphthalene - Observations NOTE: This thread is a child of the [url=http://www.sciencemadness.org/talk/viewthread.php?tid=14970 ... |
2-5-2011 at 06:54 by: m1tanker78 |
Make Potassium (from versuchschemie.de) BlogFast: Interesting result with the 2 liquid phases. I haven't observed this but then, I don't eve ... |
1-5-2011 at 13:19 by: m1tanker78 |
Synthesis of longer chain tertiary alcohols You got that right! Last night, I took the same batch from the video and heated it up to just under ... |
1-5-2011 at 10:04 by: m1tanker78 |
Make Potassium (from versuchschemie.de) [rquote=208576&tid=14970&author=blogfast25]Ok, just because it's you
I'll run a test with ... |
1-5-2011 at 09:26 by: m1tanker78 |
Sodium Garbage Time And Unusual Results 91% IPA Experiment Update:
All of the remaining IPA has evaporated, leaving only the bottom aque ... |
30-4-2011 at 17:03 by: m1tanker78 |
Make Potassium (from versuchschemie.de) Blog, I won't twist your arm but still feel like your experiment was inconclusive for the purpose of ... |
30-4-2011 at 16:27 by: m1tanker78 |
Synthesis of longer chain tertiary alcohols Blog, I coalesce Na slightly beyond the MP. After coalescence, it's good practice to ramp up the oil ... |
30-4-2011 at 15:46 by: m1tanker78 |
Synthesis of longer chain tertiary alcohols [rquote=208514&tid=15171&author=blogfast25]
In your video, I seem to see Na globules bobbin ... |
30-4-2011 at 10:46 by: m1tanker78 |
Make Potassium (from versuchschemie.de) BlogFast, straight brake fluid reacts briskly with Na as well. I assume you used straight BF for you ... |
30-4-2011 at 10:40 by: m1tanker78 |
Synthesis of longer chain tertiary alcohols Sorry about that. T'was late and I got caught up in the half-asleep excitement. ![:o](./images/smilies/shocked.gif)
Sadly, I wind ... |
30-4-2011 at 05:55 by: m1tanker78 |
Synthesis of longer chain tertiary alcohols BlogFast: Point taken about it not being a HC and about the unsuitability at higher temps.
As far ... |
29-4-2011 at 22:46 by: m1tanker78 |
Sodium Garbage Time And Unusual Results [rquote=208470&tid=16149&author=cyanureeves]yipee! i made sodium today.[...][/rquote]
Fir ... |
29-4-2011 at 15:53 by: m1tanker78 |