Thoughts On Anodes Before Xenoid suggested vibrating an anode during plating, I was already 90% done with a deluxe rota ... |
21-11-2008 at 06:57 by: Swede |
Thoughts On Anodes jpsmith, the voltage (at 15 amps) hardly varied at all throughout the run, about 6V. I think your o ... |
20-11-2008 at 06:54 by: Swede |
Thoughts On Anodes I pulled the plug on the test cell. Since this morning, there was no additional visible perchlorate ... |
19-11-2008 at 14:10 by: Swede |
Thoughts On Anodes Xenoid, that is an awesome idea! I never would have thought of that. Your rig is assembled, you ne ... |
19-11-2008 at 08:06 by: Swede |
Thoughts On Anodes Hmm, I knew it would never be as simple as I thought! Would there be ANY advantage to rotation, or ... |
18-11-2008 at 09:17 by: Swede |
Thoughts On Anodes On anode spinning - my experience with plating has been limited to decorative plating. With nickel, ... |
18-11-2008 at 08:22 by: Swede |
Thoughts On Anodes Thanks for the O3 clarification. The odd thing was, it seemed to be produced immediately, indicating ... |
17-11-2008 at 16:36 by: Swede |
Thoughts On Anodes My path to perchlorate is going to be two-step... harvest chlorate, purify (if needed) and feed pota ... |
17-11-2008 at 07:21 by: Swede |
Thoughts On Anodes I don't know the composition of the MMO. I do agree that IF (big if) it produces perchlorate with a ... |
16-11-2008 at 09:59 by: Swede |
Thoughts On Anodes I'm going to try it. I've got enough MMO mesh to equip a small country with saltwater pools. I mad ... |
16-11-2008 at 09:04 by: Swede |
Thoughts On Anodes Dann2, I think the circulation that your thermal (and H2) forces created by the setup in your drawin ... |
13-11-2008 at 17:11 by: Swede |
Thoughts On Anodes [quote][i]Originally posted by watson.fawkes[/i]
Have you consider mechanical stirring? For a cell ... |
13-11-2008 at 10:34 by: Swede |
Thoughts On Anodes @Dann2 - I wish I could continue with this run in particular, measuring chloride, and taking it very ... |
13-11-2008 at 06:57 by: Swede |
Thoughts On Anodes For fun, I've began plotting chloride concentration over time in a constant current setup. I'm usin ... |
12-11-2008 at 16:35 by: Swede |
Thoughts On Anodes Tentacles, my solubility chart shows 350 grams per liter at 25 C. Chlorine is 47.5% by weight, so t ... |
12-11-2008 at 13:09 by: Swede |
Thoughts On Anodes Tentacles, that LD plate job looks nice! And I thought MY bench was messy!
I noticed you used ... |
12-11-2008 at 06:41 by: Swede |
Thoughts On Anodes I've really been absorbing a lot of great info from you guys - I appreciate your expertise.
I've ... |
11-11-2008 at 08:12 by: Swede |
Thoughts On Anodes Rosco B, thank you for those options. I didn't even think of an irrigation sprinler. Initially I t ... |
10-11-2008 at 08:28 by: Swede |
Thoughts On Anodes I attempted to bring one of the cathodes to red heat without ruining the plastic, but it was difficu ... |
9-11-2008 at 07:21 by: Swede |
Thoughts On Anodes Tentacles, I'm inclined to agree. I've not been at this long, but all my Ti cathodes until now have ... |
7-11-2008 at 12:10 by: Swede |
Thoughts On Anodes Those cathodes were not commercially pure, if that makes a difference, they were a Ti alloy. They w ... |
7-11-2008 at 06:41 by: Swede |
Thoughts On Anodes I wheeled the collection vat outside... the cart IS the way to go for a heavy setup. I attempted to ... |
6-11-2008 at 08:32 by: Swede |
Thoughts On Anodes Well, I've got some good news, plenty of bad news. Here's what happened...
The line leading to t ... |
6-11-2008 at 08:14 by: Swede |
Thoughts On Anodes Before I can digest the evening input, I have a small situation to take care of... Why does bad ... |
6-11-2008 at 05:03 by: Swede |
Thoughts On Anodes Dann2, before I absorb your last post, I want to say - WOW - you saved my ass. As I mentioned befor ... |
5-11-2008 at 16:14 by: Swede |