Yes You Can Make Your Own TCT - If You Dare! @Maya
Sartori in THE WAR GASES (q.v.) states that BrCN slowly polymerizes to cyanuric bromide, it ... |
23-5-2007 at 17:58 by: Sauron |
Help turning chloroform to formate. You are trying to prepare normal alkyl formate esters like methyl formate, ethyl formate etc from ch ... |
23-5-2007 at 11:34 by: Sauron |
Yes You Can Make Your Own TCT - If You Dare! I reiterate: formamide is just as irrelevant as formaldehyde, to cyanuric acid, isocyanuric acid, cy ... |
23-5-2007 at 09:49 by: Sauron |
Parr Stirred Pressure Reactors On the pre-2004 Parr stirred reactors the motors are unsurprisingly 90V DC power from a 110V control ... |
23-5-2007 at 05:39 by: Sauron |
Australian power points Wise move, gambler. You want something you can actually run an entire power strip off of, rather tha ... |
23-5-2007 at 02:42 by: Sauron |
Yes You Can Make Your Own TCT - If You Dare! What leads you to conclude that cyanuric acid is a formaldehyde derivative?
Cyanuric acid is the ... |
23-5-2007 at 02:26 by: Sauron |
Lead Acetate distillation with PAA If we limit this to the classical reagents SOCl2, PCL3, POCl3, PCl5 then I would concurr.
Howeve ... |
22-5-2007 at 23:57 by: Sauron |
Australian power points @gambler
I haven't had time to look at that site yet, but I would recommend against the typical " ... |
21-5-2007 at 17:40 by: Sauron |
Australian power points Forget about "power converters" as that nomenclature is used to describe small devices to power say, ... |
21-5-2007 at 04:31 by: Sauron |
Parr Stirred Pressure Reactors There is a 4842 controller on LabX from a seller in UK called Rich-Monde but it is an older ad (not ... |
21-5-2007 at 02:29 by: Sauron |
Parr Stirred Pressure Reactors There are times when glass just won't hack it. At such times an autoclave-type "bomb" reactor is the ... |
20-5-2007 at 21:22 by: Sauron |
Preparation of Isonicotinic Acid and Ethyl Isonotinate The scheme for citric acid to citrazinic acid is on p.2 of the Potential Uses of Citric Acid thread ... |
20-5-2007 at 12:44 by: Sauron |
Potential uses of Citric Acid The rxn of ammonia with methyl or ethyl citrate to give citrazinic acid was popular in the first hal ... |
20-5-2007 at 12:39 by: Sauron |
keten lamp And I am still waiting for vinyl acetate to arrive. I think it may take substantial experimentation ... |
20-5-2007 at 00:36 by: Sauron |
Synthesis of Sulfur Trioxide and Oleum: The persulfate method @G C
Nice thread! SO3 is always of interest. The procedure you have described looks like a simpl ... |
18-5-2007 at 12:02 by: Sauron |
Call for discussion of several methods of producing pyruvic acid by dry distillation Oh true enough. Still, you would idly light your Zippo (now a fashionable antique cigarette lighter. ... |
17-5-2007 at 07:42 by: Sauron |
Call for discussion of several methods of producing pyruvic acid by dry distillation I doubt I'd use peanut oil if distilling oxidizing liquids. Silicone oil, on the other hand, is pret ... |
17-5-2007 at 07:21 by: Sauron |
Call for discussion of several methods of producing pyruvic acid by dry distillation Fine. You use a free flame in the lab. Go right ahead. Be my guest. Meanwhile I'll buy some marshmel ... |
16-5-2007 at 19:08 by: Sauron |
Call for discussion of several methods of producing pyruvic acid by dry distillation An airbath like the Kugelrohr oven for the old 4 liter model that is no longer made would be good. n ... |
16-5-2007 at 03:14 by: Sauron |
Bird Flu ?? Those might be useful for poultry workers or people who live near poultry farms or ar otherwise at r ... |
15-5-2007 at 20:35 by: Sauron |
Call for discussion of several methods of producing pyruvic acid by dry distillation @matchheads:
Right. Free flames in the lab. I guess you don't work much with ether, CS2, THF, met ... |
15-5-2007 at 20:04 by: Sauron |
PUBLIC ADVISORY: Pictures Sorry, renown is correct. No such word as 'reknown' exists in the English language. If you think oth ... |
15-5-2007 at 19:42 by: Sauron |
Bird Flu ?? It's a big problem still.
If you are a bird.
It's a nonzero risk if you are a poultry worker b ... |
15-5-2007 at 12:53 by: Sauron |
Call for discussion of several methods of producing pyruvic acid by dry distillation Often with a foaming problem like this you can handle it by switching from the 3L flask specified to ... |
15-5-2007 at 12:43 by: Sauron |
Call for discussion of several methods of producing pyruvic acid by dry distillation It's repetitious to include the Vogel procedure which he simply downsized a little from the Org.Syn. ... |
15-5-2007 at 10:14 by: Sauron |
[Next Page] |