Latest chemical order? Picked up today at Science Essentials in Brisbane:
- Formic acid 90%, AR grade, 500ml.
- Cobalt s ... |
13-8-2020 at 20:48 by: Lion850 |
Metal glycinates Hi B(a)P thank you! Even though there may not be a great interest in glycinates I think it is good t ... |
7-8-2020 at 02:33 by: Lion850 |
Metal glycinates Cobalt glycinate shed report:
I actually completed cobalt before nickel but the product took days ... |
6-8-2020 at 23:00 by: Lion850 |
Metal glycinates DraconicAcid - thanks mate. The color seems right I think. I'll search some more for a picture of th ... |
6-8-2020 at 00:31 by: Lion850 |
Metal glycinates Nickel glycinate report:
The starting materials were nickel carbonate (which I made some time ago ... |
5-8-2020 at 23:02 by: Lion850 |
Pretty Pictures (2) Salt formed from reacting nickel carbonate with glycine crystallising out on the steam bath. Hope it ... |
5-8-2020 at 18:54 by: Lion850 |
Pretty Pictures (2) A cobalt glycinate salt drying on the steam bath. The few glassy crystals is probably the slight exc ... |
4-8-2020 at 18:24 by: Lion850 |
Metal glycinates Thanks for that! Doing a google image search for copper glycinate brings up all shades of blue and e ... |
4-8-2020 at 18:05 by: Lion850 |
Metal glycinates DraconicAcid thanks for the explanation. We need for a few beers one day, so much to learn ![:)](./images/smilies/smile.gif)
Cop ... |
4-8-2020 at 17:14 by: Lion850 |
Metal glycinates Rhodanide posted a photo on his Youtube channel some 3 weeks ago showing a red chromium glycinate an ... |
3-8-2020 at 03:42 by: Lion850 |
Pretty Pictures (2) Copper glycinate crystallising out on the steam bath.
[file]82558[/file] |
1-8-2020 at 22:52 by: Lion850 |
Chromium hydroxide? I wanted to make some chromium precursor to make other chromium salts so I decided to convert some o ... |
25-7-2020 at 22:01 by: Lion850 |
Copper cyanurate (and other cyanurates} Sciece Nerd for your interest this morning I added some H2O2 drops to the filtrate from yesterday - ... |
25-7-2020 at 20:38 by: Lion850 |
Copper cyanurate (and other cyanurates} @sciece nerd Thanks for the explanation. So part of the remainder on the filter paper was fresh TiO2 ... |
25-7-2020 at 14:26 by: Lion850 |
Copper cyanurate (and other cyanurates} I did a few crude small scale double displacement reactions to see whether anything warranted furthe ... |
25-7-2020 at 02:12 by: Lion850 |
Copper cyanurate (and other cyanurates} Failures:
Chromium: I tried a few different things over many days. Chrome powder was stirred with c ... |
24-7-2020 at 17:47 by: Lion850 |
Copper cyanurate (and other cyanurates} Hi Bezaleel thanks for linking to the thread, interesting stuff. So far I was trying to get coloured ... |
17-7-2020 at 03:15 by: Lion850 |
Copper cyanurate (and other cyanurates} Cobalt continued:
The grey cobalt cyanurate salt was dried in the sun under a steel dish for 2 day ... |
17-7-2020 at 00:52 by: Lion850 |
Copper cyanurate (and other cyanurates} Cobalt:
Cobalt carbonate (see photo) was reacted with cyanuric acid to see what will happen. Reagen ... |
15-7-2020 at 02:47 by: Lion850 |
Manganese ii and iii acetates Hi Refinery - as I mentioned in the original post my first attempt also turned brown, I avoided that ... |
12-7-2020 at 17:17 by: Lion850 |
Copper Tartrate I recently acquired a bottle of old ammonium tartrate. Photo below. The lid was broken, but the cont ... |
11-7-2020 at 23:02 by: Lion850 |
Copper cyanurate (and other cyanurates} wg48temp9 - speaking under correction but I think the acid is Dichloroisocyanuric acid; if it joins ... |
11-7-2020 at 21:52 by: Lion850 |
Copper cyanurate (and other cyanurates} Woelen - it certainly looks darker on the previous photo (of the dried product) than with the eye. I ... |
10-7-2020 at 02:52 by: Lion850 |
Copper cyanurate (and other cyanurates} Manganese:
I had a go at reacting manganese powder with cyanuric acid. According to "Cyanuric Acid ... |
10-7-2020 at 00:47 by: Lion850 |
Pretty Pictures (2) Interesting color I thought for a copper salt (that does not contain another metal, only copper). A ... |
7-7-2020 at 13:14 by: Lion850 |