Making Pinchbeck Brass Another promising option is [b]aluminum bronze[/b], a mixture of about 90% copper and 10% aluminum. ... |
25-4-2018 at 03:58 by: MrHomeScientist |
Making Pinchbeck Brass I found this neat graphic on this site: http://cascadecoil.com/2014/12/gold-silver-bronze-your-guide ... |
23-4-2018 at 13:48 by: MrHomeScientist |
How toxic is methanol actually? If I ever spill methanol on my skin, I go take a shot of rum just in case |
23-4-2018 at 07:56 by: MrHomeScientist |
Making Pinchbeck Brass I did; some borax before each zinc addition. Perhaps not enough?
[Edited on 4-23-2018 by MrHomeScie ... |
22-4-2018 at 19:20 by: MrHomeScientist |
Making Pinchbeck Brass I finished off the brass series this weekend by adding two new ingots to the collection. Same proced ... |
22-4-2018 at 16:14 by: MrHomeScientist |
Fun Phosphorus Speculations [rquote=515014&tid=82090&author=Magpie]Stench is no problem, just turn on the hood fan.
I ... |
20-4-2018 at 10:22 by: MrHomeScientist |
Fun Phosphorus Speculations I think it's interesting to compare the above process for making phosphorus to the ones being done i ... |
20-4-2018 at 06:50 by: MrHomeScientist |
What is cause of global warming? Heat or gases? He (and I) are trying to point out that your chart:
[file]67502[/file]
clearly shows that the ... |
18-4-2018 at 09:55 by: MrHomeScientist |
What is cause of global warming? Heat or gases? [rquote=514628&tid=81554&author=byko3y][b]MrHomeScientist[/b]Ocean contains approx 40 000 gi ... |
17-4-2018 at 11:59 by: MrHomeScientist |
What is cause of global warming? Heat or gases? I'm reluctant to butt in, but if I understand that picture correctly the up arrows are carbon releas ... |
17-4-2018 at 07:07 by: MrHomeScientist |
The trouble with neodymium... I ran into a similar problem. We found that just adding the [u]solid[/u] K[sub]2[/sub]SO[sub]4[/sub] ... |
17-4-2018 at 05:35 by: MrHomeScientist |
Google's search results have changed drastically! Because he's trying to acquire reagents and apparatus from online suppliers?
I haven't noticed an ... |
16-4-2018 at 10:02 by: MrHomeScientist |
Mercury...again [rquote=514473&tid=81923&author=XeonTheMGPony]
Old medical offices some even pay me to ta ... |
16-4-2018 at 06:10 by: MrHomeScientist |
The trouble with neodymium... Doesn't look like anyone knows! Unfortunately blogfast isn't around currently to answer. Perhaps som ... |
16-4-2018 at 06:02 by: MrHomeScientist |
Making Pinchbeck Brass I did some more calculations on my results. It gets a little complicated!
tl;dr - I was aiming fo ... |
15-4-2018 at 14:53 by: MrHomeScientist |
Making Pinchbeck Brass I had trouble getting a nice picture of the samples too. It's hard to capture the true colors. In th ... |
15-4-2018 at 05:53 by: MrHomeScientist |
Making Pinchbeck Brass Good luck, EC1! Alloying pennies together is a great idea. The consistent masses between pennies sho ... |
14-4-2018 at 19:26 by: MrHomeScientist |
Making Pinchbeck Brass Is the borax added before or after melting? Before adding zinc? Should it be dehydrated first or jus ... |
13-4-2018 at 12:19 by: MrHomeScientist |
Making Pinchbeck Brass From the SA article I linked:
[quote]First, melt the least fusible of the metals (that requiring th ... |
12-4-2018 at 12:55 by: MrHomeScientist |
Making Pinchbeck Brass EC1, that's really great information! Thanks for taking the time to post all that. That supports my ... |
12-4-2018 at 09:30 by: MrHomeScientist |
Isolation of barium metal from baryte sample Aluminum may not work as you think it would. The change in enthalpy is extremely positive at 1172 kJ ... |
10-4-2018 at 11:41 by: MrHomeScientist |
Isolation of barium metal from baryte sample I could have sworn there was a thread here on this topic, but I can't find it right now. If I rememb ... |
10-4-2018 at 10:08 by: MrHomeScientist |
Reduction of KCr(SO4)2 Not sure about the pottery stuff; I've never had access to a good pottery supplier. My intuition say ... |
10-4-2018 at 05:35 by: MrHomeScientist |
Making Pinchbeck Brass When should the flux be added? Before or after melting? How much flux per melt? I assume it needs to ... |
9-4-2018 at 12:42 by: MrHomeScientist |
Reduction of KCr(SO4)2 Awesome! Was your sulfur mixed throughout as a heat booster, or did you just use it in a pile on top ... |
9-4-2018 at 12:33 by: MrHomeScientist |