Search |
HCl from common fertilizers Oops. I meant K2CO3 to produce K2SO4 and not NaCl.
Sorry. |
25-11-2002 at 10:24 by: BASF |
HCl from common fertilizers I am quite aware of teh fact, that Na2SO4 would be really really cheap, as it can be produced at ver ... |
25-11-2002 at 10:20 by: BASF |
HCl from common fertilizers You might have a point there, but the electrolysis of NaCl followed by burning the gases is the best ... |
22-11-2002 at 09:24 by: BASF |
HCl from common fertilizers
1/2Na2SO4 + 1/2(NH4)2SO4 <> NaNH4SO4
Somebody has to write a good manual for the prod of HCl o ... |
19-11-2002 at 17:23 by: BASF |
methanol from CO2 Thanks for your input, but i think i`d better keep my acetonitrile for other purposes;-) |
15-11-2002 at 10:38 by: BASF |
Phorone Yes, there was fizzling.....it was (as expected) a very vigorous reaction.
The addition had to be d ... |
14-11-2002 at 10:58 by: BASF |
ppt reactions for H2SO4 out of fertilizers I was once dreaming of making a solar powered sulfuric acid generator that uses the common ammonium ... |
13-11-2002 at 17:54 by: BASF |
HCl from common fertilizers (NH4)2SO4>NH3 + NH4HSO4
NH4HSO4 + NaCl>1/2Na2SO4 + HCl
+ 1/2(NH4)2SO4
The hot HCl gas could ... |
13-11-2002 at 17:19 by: BASF |
Phorone what the fuck.....did anyone try to import photos yet?
....u can still paste the urls....sorry |
13-11-2002 at 16:01 by: BASF |
phorone-batch with photos A) A batch consisting of 30mL 30% HCl and 20mL of commercial acetone in a loosely stoppered flask w ... |
13-11-2002 at 15:58 by: BASF |
Can't make CuO you want to get pure CuO, right?
Make a solution of CuSO4, then add a mix of NaOH and H2O2.
Blac ... |
13-11-2002 at 11:07 by: BASF |
Diphoronepentaperoxide (DPPP) My god THATS good news.....1,0-1,3g/mL is the density of the peroxidation product i obtained recentl ... |
9-11-2002 at 06:19 by: BASF |
from camphor?? Phorone
(Phor"one) n. [Camphor + acetone.] (Chem.) A yellow crystalline substance, having a geraniu ... |
8-11-2002 at 10:40 by: BASF |
Self-condensation of acetone Text from
http://www.library.uu.nl/digiarchief/dip/diss/1977553/c1.pdf
The Self-Condensation ... |
8-11-2002 at 10:14 by: BASF |
Diphoronepentaperoxide (DPPP) DBSP
I read the posts on E&W, but i can say that the inventor definitely didnt mean 9000ft/s inst ... |
8-11-2002 at 07:37 by: BASF |
conc. sulfuric acid with acetone Polverone: If u want u can pass some of the articles to me for translation, i speak german.
25mL ... |
6-11-2002 at 16:30 by: BASF |
Diphoronepentaperoxide (DPPP) I am not very confident that the obtained product contains much phorone as it is non soluble in orga ... |
6-11-2002 at 15:37 by: BASF |
Diphoronepentaperoxide (DPPP) 1) 25mL of 30% HCl were added to 75mL of acetone and treated like in C) of the previous post.
Yie ... |
5-11-2002 at 15:32 by: BASF |
Reactions of acetone with HCl I spent two weekends doing this....
1) A) A batch consisting of 30mL 30% HCl and 20mL of commerci ... |
5-11-2002 at 14:34 by: BASF |