Making Lead Nitrate
Don't forget the Lead Salts Preparation thread.

http://www.sciencemadness.org/talk/viewthread.php ...
24-6-2014 at 12:19
by: jock88
Making Lead Nitrate

Had a similar problem. The SOS I think is Tin Oxide.
The 'Lead' sheet may be old and contain Tin ...
23-6-2014 at 14:22
by: jock88
Perchlorate chemistry

Is this available to anyone?

http://books.google.ie/books/about/Perchloric_acid.html?id=GzAaAQA ...
23-6-2014 at 14:06
by: jock88
Short question / quick answer - Thread

Try this

http://oxidizing.typhoonguitars.com/chlorate/mag_chlorate.html

18-6-2014 at 15:16
by: jock88
Question on setup of electrochemical cell

I think a guy who posts here (Burner?) is going to try some in the near future and report back. ;)
17-6-2014 at 14:54
by: jock88
What could Benzene be worth, sold by the liter.

Depends on purity. If selling stuff that is research grade (99.99 or whatever) then it's going to ...
17-6-2014 at 14:39
by: jock88
Source for Merbromin

Thanks for replys.
It's available on ebay as solution:

http://www.ebay.co.uk/itm/Merbromin-2-a ...
17-6-2014 at 14:37
by: jock88
Source for Merbromin

Looking for Merbromin (pure powder).

http://en.wikipedia.org/wiki/Merbromin

Any know of a so ...
16-6-2014 at 14:42
by: jock88
Vanadium: The metal that may soon be powering your neighbourhood

The energy is actually stored in the electrolyte. The capacity of the battery in dictated by how m ...
15-6-2014 at 12:34
by: jock88
Great Online Chemistry Texts for the Beginner and the Curious!
http://www.drkfs.net/

Looks like a useful site.
13-6-2014 at 13:23
by: jock88
self-made high-vacuum diffusion pump
Homemade Pirani gauge here

http://www.drkfs.net/pirani.htm

13-6-2014 at 13:21
by: jock88
Decent laboratory balances?
Any thoughts on these contraptions?

http://www.ebay.co.uk/itm/Stanton-CL14-1970s-Vernier-Scientif ...
7-6-2014 at 15:59
by: jock88
The lead salts preparation thread!
Leas salts thread:

http://www.sciencemadness.org/talk/viewthread.php?tid=5490
6-6-2014 at 05:10
by: jock88
Any lead sulfate reactions?
Leas salts thread:

http://www.sciencemadness.org/talk/viewthread.php?tid=5490
6-6-2014 at 05:09
by: jock88
Any lead sulfate reactions?
"
Now, PbSO4 is highly insoluble, but solubility is always relative. Lead sulfate has a Ksp of 2.53 ...
5-6-2014 at 14:20
by: jock88
Just had cops show up

Thats a sweet copper you persuaded the sheriffs department to leave with you arkoma. Whats that fu ...
3-6-2014 at 03:06
by: jock88
The Short Questions Thread (4)

I think noodles are the new boiling chips.
3-6-2014 at 02:53
by: jock88
Fused Quartz furnace

You can obtain fuzed quartz tubes from the dumpster. They are contained in some domestic radiant h ...
3-6-2014 at 02:51
by: jock88
Making Nitrates


This method might fill the void:

http://www.sciencemadness.org/talk/viewthread.php?tid=25829
3-6-2014 at 02:44
by: jock88
Exotic thermites & analogs
http://www.popularmechanics.com/technology/military/research/the-ultrahot-torch-that-slices-through- ...
1-6-2014 at 11:44
by: jock88
The Short Questions Thread (4)

http://oxidizing.typhoonguitars.com/

Current density at the anode is:
current into cell divi ...
31-5-2014 at 04:11
by: jock88
Gore-Tex as a cell membrane

Have you got anything against the auld blunt fellas?

http://www.ebay.co.uk/itm/Sheet-of-DPM-Gor ...
30-5-2014 at 13:17
by: jock88
Glass adapter pieces to put a flask under pressure?

If you can spare some glass and you have spare glass you could set up with just water at 130C or p ...
30-5-2014 at 13:09
by: jock88
Sciencemadness comment box!
Because those threads/subforums are deemed to be serious before hand.

24-5-2014 at 12:48
by: jock88
Drying ethanol.

I seen a procedure way back in time regarding making super-dry ethanol.
First you distilled using ...
18-5-2014 at 05:59
by: jock88
[Next Page]

  Go To Top