Can’t do brazing I figured it out, that guy was right when he said the flame was reducing the metal. I understand tha ... |
28-9-2018 at 15:51 by: Stealthsilent |
Can’t do brazing Please read what I was trying to do.
Are you sure it’s shiny because it’s being reduced by th ... |
25-9-2018 at 03:18 by: Stealthsilent |
Can’t do brazing So this is me melting tin, ignore the audio, it’s just me babbling.
You’ll notice the tin glo ... |
24-9-2018 at 22:10 by: Stealthsilent |
Can’t do brazing Interesting, thank you for your responses. I want to understand what is going on, that’s why I’m ... |
14-9-2018 at 18:40 by: Stealthsilent |
Can’t do brazing I’m trying to melt some metals into other metals and I’m trying a bunch of different reducing ag ... |
13-9-2018 at 17:00 by: Stealthsilent |
Update: selling equipment and reagents If you could sell me the hot plate for 30$, I’ll buy it. |
2-9-2018 at 18:57 by: Stealthsilent |