Search |
[Next Page] |
How to [recover] dissolved in acid Tin Sorry guys, too many of you asked too many questions all at once, I'm confused.
Displaced Sn with A ... |
9-6-2024 at 19:06 by: Romix |
How to [recover] dissolved in acid Tin [rquote=693469&tid=160363&author=Sulaiman]As above, tin electrolysis is super easy,
Blatan ... |
8-6-2024 at 11:31 by: Romix |
How to [recover] dissolved in acid Tin [rquote=693459&tid=160363&author=bnull]Did you try electrolysis?[/rquote]
Not yet. |
7-6-2024 at 15:52 by: Romix |
How to [recover] dissolved in acid Tin Hello again Dear forum members.
Any literature you could recommend?
Or maybe you have experience ... |
7-6-2024 at 15:40 by: Romix |
NPK from incinerated bones Yes, did something wrong the first time I did it, probably not put enough of Ammonium Molybdate in i ... |
17-5-2024 at 21:20 by: Romix |
NPK from incinerated bones [rquote=693087&tid=160317&author=bnull][rquote=693085&tid=160317&author=Romix]Bullsh ... |
15-5-2024 at 10:49 by: Romix |
NPK from incinerated bones [rquote=693068&tid=160317&author=Romix]I should receive 25g of Ammonium Molybdate in the ne ... |
15-5-2024 at 08:52 by: Romix |
NPK from incinerated bones I should receive 25g of Ammonium Molybdate in the next couple of days.
First I'll test it on K2HP ... |
14-5-2024 at 07:01 by: Romix |
NPK from incinerated bones Carbon that settled when I've poured water of it, I've put in a pot with massive fig tree, it seems ... |
14-5-2024 at 00:04 by: Romix |
NPK from incinerated bones First crystals out of dissolved bones...
[file]101911[/file]
[Edited on 14-5-2024 by Romix] |
13-5-2024 at 18:07 by: Romix |
NPK from incinerated bones [rquote=692999&tid=160317&author=bnull][rquote=692952&tid=160317&author=Romix]What d ... |
13-5-2024 at 17:29 by: Romix |
NPK from incinerated bones [rquote=693019&tid=160317&author=Romix]And would this yellow precipitate form if any Phospha ... |
11-5-2024 at 09:49 by: Romix |
NPK from incinerated bones And would this yellow precipitate form if any Phosphate would be present in a solution full of Alkal ... |
11-5-2024 at 03:56 by: Romix |
NPK from incinerated bones [rquote=692995&tid=160317&author=Romix]Is this is a good reaction for Phosphate anions in so ... |
11-5-2024 at 03:53 by: Romix |
NPK from incinerated bones bnull thank you for the link, I like the prices, not bad... not seen the postage fees yet... Also I ... |
10-5-2024 at 01:11 by: Romix |
NPK from incinerated bones After burning all organics out of the bones in a set up like on a picture above, rest of carbon can ... |
9-5-2024 at 22:12 by: Romix |
NPK from incinerated bones [rquote=692999&tid=160317&author=bnull][rquote=692952&tid=160317&author=Romix]What d ... |
9-5-2024 at 21:59 by: Romix |
NPK from incinerated bones Any predictions what could dry Alkali Acetates decompose into at very high temperatures?
Like gas, ... |
9-5-2024 at 19:14 by: Romix |
NPK from incinerated bones Is this is a good reaction for Phosphate anions in solution??? Maybe you could recommend alternative ... |
9-5-2024 at 18:58 by: Romix |
NPK from incinerated bones Carbon that absorbed some of the nutrients while dissolving bones can be sprinkled in the soil... In ... |
9-5-2024 at 18:29 by: Romix |
NPK from incinerated bones Is it possible to produce Phosphoric acid out of them? |
9-5-2024 at 18:07 by: Romix |
NPK from incinerated bones Sample, will try remove more carbon out of them tomorrow in a day time... I thought it will smell mu ... |
9-5-2024 at 17:47 by: Romix |
NPK from incinerated bones So if this reactions with HNO3 will work, your advise about use of NH4OH and its dissolving cations ... |
9-5-2024 at 17:44 by: Romix |
NPK from incinerated bones Are these reactions correct?
Ca3(PO4)2 + 2HNO3 ⇄ Ca(NO3)2 + 2CaHPO4
2CaHPO4 + 2HNO3 ⇄ Ca(NO3) ... |
9-5-2024 at 17:35 by: Romix |
NPK from incinerated bones Been told, that reactions might even go with weak acetic acid instead of HCl.
Like that Ca3(PO4)2 + ... |
7-5-2024 at 21:46 by: Romix |